Nestor J. Zaluzec, a senior scientist at the U.S. Department of Energy’s (DOE) Argonne National Laboratory, has been named an inaugural Fellow in the Legends Class of the Microanalysis Society, in recognition of his contributions to advanced microscopy and microanalysis.
Studying crack propagation with 3D imaging
A Texas A&M University research team has taken the first 3D image of a microscopic crack propagating through a metal damaged by hydrogen. The new research shows what is happening at the crack tip as a part begins to fracture. The team identified 10 microscopic structures that make metals stronger and less susceptible to hydrogen embrittlement.
MIPAR software enables precise and repeatable quantification of nickel alloy precipitates
Covalent Metrology announces collaboration with Edax on energy dispersive spectroscopy
ASM International CEO Corner: Impact Factors on the Rise for ASM Journals
Impact Factors on the Rise for ASM Journals