Iowa State University and its Ames Laboratory report that researchers have received a three-year, $2.8 million grant to develop a ductile electrical steel containing 6.5% silicon, twice the amount in electric motor steel today.
Most titanium is now made by the Kroll process, in which titanium dioxide is reacted with chlorine to form titanium etrachloride, which is then reacted with magnesium to strip away the chlorine and leave behind the pure metal.
Thermo-Calc Software AB, Stockholm, and QuesTek International LLC, Evanston, Ill., have partnered to establish a joint company, QuesTek Europe AB, which will offer Integrated Computational Materials Engineering modeling services and novel materials design and development to the European market.