Nanostructured zinc nickel coating system for oil and gas industries

July 6, 2022
Source: ASM International

Integran Technologies, Inc., Canada, Dipsol of America, Inc, Livonia, Michigan, and Sigma Fasteners, Inc., Houston, TX, announce their agreements to expand access to Nanostructured Zinc-Nickel fastener and bolting products for the oil and gas industries worldwide.

ZNnGard replaces toxic plating in addition to other organic coatings that easily chip and flake under torque and require oversized nuts with a sustainable alloy coating that gives a superior performance during installation and long-term corrosion protection. Integran originally developed the pulse-electro deposition process in 2011 with support from the Department of Defense Strategic Environmental Research and Development Program as an environmentally friendly cadmium-replacement coating for high-strength steel.   

Sigma Fasteners, Dipsol, and Integran have worked together to bring the Nanostructured Zinc Nickel coating system to the Oil and Gas Industries. ZNnGard meets the requirements of the ASTM B841 Class 2 as an electrodeposited zinc-nickel alloy coating on fasteners. Integran Technologies is the master licensor for its Nanovate Zn-Ni Technology and intellectual property owner in waveform pulse plating technologies. Dipsol America is the master distributor for the expressly branded ZNnGard and ZNnCoat chemistry and components for plating and chromate finish. Sigma Fasteners, a leader in energy bolting, will use this expertise in converting its current Zn-Ni line to meet Integran standards and Dipsol chemistries to ramp up advanced field testing and production in Houston.

 

Image – ZnGard bolts. ZNnGard, a Zinc-Nickel nanostructured electroplating system that is considered part of an overall strategy to replace cadmium, PTFE, ceramic metallic, and fluoropolymer processes, eliminate environmental and worker safety issues while significantly improving performance and reducing life-cycle costs.

 

For more information:

Dipsol of America, Inc.

http://www.dipsolamerica.com/

 

Integran Technologies, Inc.

https://www.integran.com/

 

Sigma Fasteners, Inc.

https://www.sigmafasteners.com

 

Subject Classifications

Fossil Fuel Power

Industries and Applications

Materials Processing and Treatment

Metals and Alloys

news

News Articles

Uncategorized