Seco/Warwick, Meadville, PA announced that their previous furnace with an aviation industry client will be retired and replaced by a new, economical, and versatile furnace for brazing jet engine parts.
Seco/Warwick has been a recognized metal heat treatment equipment manufacturer for decades. In fact in many plants, units were manufactured in the 1980s and 1990s. The partners are gradually replacing these units with modern solutions, continuing to be loyal to the SECO/WARWICK brand.
“The aviation industry is a very important partner that has been cooperating with Seco/Warwick for decades. This is proof of satisfaction with the products we create, but also an expression of trust. Long-term, strategic, good relationships are key. Our furnaces are designed to operate without failure for many, many years, as evidenced by the replacement of this furnace after so many years,” said Maciej Korecki, vice president of the Vacuum Furnaces Segment at Seco/Warwick Group.
The new solution is based on a standard Vector vacuum furnace with a working space of 900x900x1200 mm, equipped with screen insulation and metal heating elements. It has been specifically adapted to meet the unique needs of the aviation industry, capable of heat treating complex jet engine components such as gears and main shafts.
This latest advancement underscores Seco/Warwick’s dedication to innovation and excellence, ensuring their continued partnership with the aviation industry for years to come.