ASM Industry News

ASM Industry News 

Web Content Listing

IMT’s eight-Inch wafer fabrication capabilities double the number of devices per wafer

June 19, 2019

Innovative Micro Technology Inc. (IMT), Santa Barbara, Calif., announces that it is now offering eight-inch (200mm) wafer fabrication capabilities, thereby improving the economics of MEMS production by yielding roughly twice the number of devices per wafer.

News, Magazine & Media / Industry News

Norsk Titanium completes Boeing Materials Allowables, 3D prints Questek titanium wire

June 19, 2019

Norsk Titanium, Norway, announces the successful completion of the latest phase of Boeing’s rigorous Material Allowables Program, which characterizes the titanium alloys manufactured by the AM rapid plasma deposition process.

News, Magazine & Media / Industry News

Lawrence Berkeley Lab develops map of possible stable ternary nitride compounds

June 19, 2019

Lawrence Berkeley Lab, Calif., in close collaboration with the National Renewable Energy Laboratory and other institutions, has developed a large interactive stability map of the ternary nitrides, highlighting nitride compositions.

News, Magazine & Media / Industry News

ASM International forms partnership with JobsOhio to enhance its Additive Manufacturing Training Program

June 18, 2019

JobsOhio has partnered with ASM International in the form of a nonprofit contribution to enhance the additive manufacturing knowledge of Ohio-based companies. The decision to engage with ASM International comes after a discovery process that was championed by Team NEO. The contribution of $475,000 will be utilized specifically for ASM’s Additive Manufacturing Training Program to add...

News, Magazine & Media / Industry News

Carpenter Technology, BMT Aerospace partner to produce additively manufactured parts

June 17, 2019

Carpenter Technology Corp., Philadelphia, and Belgium-based BMT Aerospace announce that they are cooperating in the development of an additively manufactured aerospace pinion made of Carpenter’s Custom 465 Stainless.

News, Magazine & Media / Industry News

Dept. of Energy to invest $32 million in projects to develop new functional materials

June 17, 2019

The U.S. Department of Energy, Washington, announces that it will invest $32 million over the next four years to accelerate the design of new materials through use of supercomputers.

News, Magazine & Media / Industry News

EWI additive manufacturing projects include alloys, powders, processes, testing

June 17, 2019

Edison Welding Institute (EWI), Columbus, Ohio, announces that its Additive Manufacturing Consortium (AMC) research projects for 2019 include studies of Inconel 625 and 718, powder measurement techniques, surface finishing, and more.

News, Magazine & Media / Industry News

Solar Atmospheres 14-foot car-bottom air furnace can treat loads up to 30,000 pounds

June 13, 2019

Solar Atmospheres of Western PA, Hermitage, recently installed a 14-foot long car bottom air furnace for the tempering of large tool steel components, as well as the age hardening processes of nickel-based alloys and precipitation hardenable stainless steels.

News, Magazine & Media / Industry News

Seco Warwick introduces new integral quench furnace and gas quench system

June 13, 2019

Seco Warwick, Meadville, Pa., introduces its Super IQ integral quench furnace and UCM 4D Quench system.

News, Magazine & Media / Industry News

One Minute Mentor: Martensitic heat treating

June 12, 2019

The graph shows the tempering response of hardened 52100 bearing steel.

News, Magazine & Media / Industry News