Vacuum Heat Treating, June 24-25, 2019

June 24, 2019 - June 25, 2019
Venue: ASM World Headquarters - Materials Park | Location: Novelty, OH, 44073-0002
Instructor: Virginia Osterman, PhD, FASM | Classroom | Product code: I-00018758

Price: $1600.00 Member Price: $1400.00

Class Dates

Oct 28, 2019 - Oct 29, 2019 Venue: ASM World Headquarters - Materials Park Location: Novelty, OH, USA Instructor: Virginia Osterman, PhD, FASM


This course teaches the background and practical applications of vacuum furnace heat treating. The student will be introduced to the fundamentals of vacuum furnaces and related system components. A complete understanding of vacuum measurement and vacuum pumping systems needed to perform various vacuum heat treating processes will be reviewed. This course provides a practical understanding of vacuum technology as related to heat treating and is as a follow up to courses which cover the fundamental metallurgy of what happens when metals are heated and cooled. This course will include hands on instruction utilizing the new ASM Laboratory Vacuum Furnace and include examples of real world heat treating cycles.

Solar Atmospheres "Mentor"Vacuum Technology focuses on:

  • Vacuum fundamentals
  • Partial pressure
  • Vacuum furnace designs
  • Vacuum furnace operation
  • Pumping systems
  • Vacuum furnace maintenance
  • Vacuum furnace heat treating processes
     

LEARNING OBJECTIVES:

Upon completion of this course, attendees can:

  • Name the advantages of vacuum heat treating compared to conventional atmospheric heat treating
  • List the basic types of vacuum furnaces
  • Explain how vacuum furnaces are insulated, heated, regulated, cooled, and evacuated
  • Explain the basics of operating a vacuum furnace
  • Explain the basic maintenance procedures to maintain a vacuum furnace
  • Discuss the advantages of vacuum heat treating compared to conventional atmospheric heat treating
  • Describe four surface treatments that make use of vacuum technology
  • Describe how vacuum furnaces are used in the heat treating of tool steels, stainless steels, Inconel® 718, titanium and its alloys
  • Be able to design a basic vacuum heat treat cycle for age hardening, solution annealing, and simple brazing.
     

WHO SHOULD ATTEND

  • Plant managers/supervisors
  • Furnace operators
  • Metallurgists, engineers, and technicians
  • Quality control personnel
  • Sales and marketing personnel
     

SUGGESTED PREREQUISITES

High school chemistry and physics would be helpful.

Continuing Education Units: 1.5

Further Your Knowledge


MATERIAL RESOURCES

Vacuum Heat Treating, October 28-29, 2019

Oct 28, 2019 - Oct 29, 2019

Virginia Osterman, PhD, FASM

ASM World Headquarters - Materials Park,
Novelty, OH, USA

Practical Heat Treating, October 7-10, 2019

Oct 07, 2019 - Oct 10, 2019

Mr. William L. Mankins, FASM

ASM World Headquarters - Materials Park,
Novelty, OH, USA

Heat Treating Furnaces and Equipment, November 14-15, 2019

Nov 14, 2019 - Nov 15, 2019

Mr. Stephen A. Maus

ASM World Headquarters - Materials Park,
Novelty, OH, USA