Component Design

Author: M. Solari, CTI Consultores de Tecnologi┬┤a e Ingenieri┬┤a SRL; P. Bilmes, Universidad Nacional de La Plata    |   Document Download   |   Product code: ZFAHT2008P001

File size: 1 MB

Classified as: Environmental Impacts Industrial Design ...more

Price: $ Member Price: $20.00

Design involves different creative aspects: planning, development, procedures, availability, and fitness concerning the materials and processes used to manufacture the component. Design is an iterative process, often based on experience, to provide an assessment of the performance of a component for a certain period of time of expected or intended service life. The design process culminates in a technical specification for the part or system and suitable manufacturing processes. Another obvious aim of design is to prevent failures throughout the component lifetime cycle and avoid situations resulting in severe failure.

  • From: Failure Analysis of Heat Treated Steel Components (ASM International)
  • Published: September 01, 2008
  • Pages: 42