Mechanical and Infrared Thermography Analysis of Shape Memory Polyurethane

Author: Elzbieta Alicja Pieczyska, Michal Maj, Katarzyna Kowalczyk-Gajewska, Maria Staszczak, Institute of Fundamental Technological Research PAS, Hisaaki Tobushi, Aichi Institute of Technology, Shunichi Hayashi, SMP Technologies Inc., Mariana Cristea, Institute of Macromolecular Chemistry    |   Document Download   |   Product code: ZCP2013SMST282

File size: 182 KB

Free to Members
Initial experimental evaluation of a new polyurethane shape memory polymer (PU-SMP) subjected to uniaxial tension carried out at different strain rates is presented. The stress and strain data were recorded and temperature changes from the SMP specimen surface was determined using fast and sensitive infrared camera. Basing on the mechanical characteristics and their relevant temperature changes, the SMP thermomechanical properties have been studied. Influence of the strain rate on the SMP temperature, its structure and behaviour are discussed. Identification of the PU-SMP parameters for one-dimensional rheological model proposed by Tobushi et. al. will be performed.
  • From: SMST-2013:The International Conference on Shape Memory and Superelastic Technologies (SMST) (ASM International)
  • Publisher: ASM International
  • Published: May 01, 2013
  • Pages: 2