ITSC 2019 abstract: Deposition of silicon carbide based coatings using high velocity oxy-fuel spraying

April 05, 2019

Development of a new SiC-based powder has enabled the deposition of dense silicon carbide coatings using thermal spraying techniques for the first time.

News, Magazine & Media / Industry News

Spray Tips: Selective galvanizing by cold spray

April 03, 2019

Cold spraying has been found to be a useful approach for the selective protection of localized areas that are the likely locations for corrosive attack, as shown in the diagram.

News, Magazine & Media / Industry News

Ametek Land develops infrared spot pyrometer for galvannealed steel strip temperature

April 03, 2019

Ametek Land, England, has been selected as a finalist in the seventh annual S&P Global Platts Global Metals Awards in the “Breakthrough Solution of the Year” category for its innovative new Spot GS (galvannealed and galvanized strip), an advanced noncontact infrared spot pyrometer.

News, Magazine & Media / Industry News

Oerlikon acquires TeroLab Surface GmbH to expand portfolio of coating services

April 03, 2019

Oerlikon, Switzerland, announces that it has acquired TeroLab Surface GmbH to expand Oerlikon Metco’s coatings services by increasing market applications and service accessibility to customers.

News, Magazine & Media / Industry News

Metalysis announces Gen4 commercial production of titanium by Cambridge process

April 03, 2019

Metalysis, England, announces that the United Kingdom’s Defence Science and Technology Laboratory (Dstl), part of the Ministry of Defence, has become a customer for its titanium powder through the Materials for Strategic Advantage research program.

News, Magazine & Media / Industry News

Spray Tips: Selective galvanizing by cold spray

March 31, 2019

Cold spraying has been found to be a useful approach for the selective protection of localized areas that are the likely locations for corrosive attack, as shown in the diagram.

News, Magazine & Media / Industry News

Rigaku EDXRF instrument analyzes elements from Na through U in almost any matrix

March 21, 2019

Rigaku, Japan, announces the newest addition to the NEX DE series, the Rigaku NEX DE VS direct excitation variable-spot EDXRF elemental analyzer, which is uniquely suited for small spot analysis applications.

News, Magazine & Media / Industry News

Plasma-enhanced titanium and vanadium nitrides form hardest thin films ever

March 12, 2019

Lehigh University, Pa., announces that its researchers have developed plasma-enhanced atomic layer deposited titanium and vanadium nitrides that are said to be harder than commercial coatings “by orders of magnitude.”

News, Magazine & Media / Industry News

Asylum Research Jupiter AFM provides 200-mm sample access and higher resolution

March 11, 2019

Oxford Instruments Asylum Research, Santa Barbara, Calif., announces the new Jupiter XR Atomic Force Microscope, the first and only large-sample AFM to offer both high-speed imaging and extended range in a single scanner.

News, Magazine & Media / Industry News

Kermetico makes specialized HVAF systems for a wide variety of powders and substrates

March 08, 2019

Kermetico, Benicia, Calif., makes specialized HVAF systems to spray metal coatings and alloyed powder compositions onto uncommon substrates such as acme threads, thin walls, and temperature-sensitive materials.