Wisconsin Oven, East Troy, WI, announces that it has shipped an Electrically Heated Drop Bottom Furnace with a traveling quench tank and maintenance platform to the aerospace industry. This system will be used for the solution heat treatment of aluminum parts.
The drop bottom furnace has a maximum operating temperature of 1,100°F and effective workspace dimensions of 3’6” W x 3’6” L x 4’0” H. An OSHA-compliant maintenance platform provides ease of access for personnel to service the equipment. The quench tank has a capacity of approximately 1,700 gallons and includes fluid level control (low, fill, high), a lockable water drain port at the bottom of the tank, and an agitator for water circulation. The traveling quench tank is enclosed with safety fencing for added safety during operation.
This drop bottom furnace is designed with sufficient capacity to heat 600 pounds of aluminum per load and provide a quench delay that does not exceed 5 seconds. The system also includes a slow drop speed program for heating applications that do not require a quench. A video of this system in operation can be viewed online.
“This drop bottom furnace was designed with a 5-second quench delay and a temperature uniformity of +/- 5°F at the set points 850°F and 1,100°F. Additionally, the system was tested to be in compliance with AMS 2750F, Class 1 furnaces, and Instrumentation Type C prior to shipment from our manufacturing facility,” said Mike Grande, Vice President of Sales.