Skip to content

One Minute Mentor: Controlled Atmosphere Furnace Equipment

Heat treatment of tool steels usually requires high flexibility combined with small lots of parts. Seal quench furnaces, executed with a single heating chamber, meet this demand. Figure 5 shows a typical schematic of a single-chamber furnace, executed with a pre-chamber, which is used both for loading and unloading and also for oil quenching or gas cooling. Another execution is shown in Fig. 6, where the load is fed directly into the heating chamber (left side in the drawing). In this case the load is transported through the furnace and received after oil quenching on the right-hand side.

For more information, click on the link below (subscription required). Then scroll to Figure 5.

R Schneider; R. Mesquita; W Schützenhöfer, Distortion in Tool Steels, ASM International, 2014, https://doi.org/10.31399/asm.hb.v04d.a0005958