Ames Laboratory, Ames, Iowa, announces that it will play a key role in the Lightweight Materials National Lab Consortium, which is dedicated to developing cleaner, cheaper, smarter, stronger, lighter, and more corrosion-resistant materials for industry.
Continue readingBioresorbable magnesium alloy shows promise as coronary scaffold
Magnesium Elektron, U.K., announces that a ten-year research program with Biotronik, Germany, has resulted in Elektron’s SynerMag 410 alloy system being selected as the platform material in the Biotronik magnesium coronary scaffold.
Continue readingAlcoa chooses the name Arconic for its future value-add company
Alcoa, Pittsburgh, announces that the name for its future company dedicated to value-added products will be Arconic, where “A” represents Alcoa, “arc” represents the arc of progress, and “-conic” speaks to the company’s history of creating iconic products.
Continue readingAlcoa chooses the name Arconic for its future value-add company
Alcoa, Pittsburgh, announces that the name for its future company dedicated to value-added products will be Arconic, in which “A” represents Alcoa, “arc” represents the arc of progress, and “-conic” speaks to the company’s history of creating iconic products.
Continue readingAlcoa chooses the name Arconic for its future value-add company
Alcoa, Pittsburgh, announces that the name for its future company dedicated to value-added products will be Arconic, in which “A” represents Alcoa, “arc” represents the arc of progress, and “-conic” speaks to the company’s history of creating iconic products.
Continue readingDirect gas-fired ovens temper tire molds for auto industry supplier
Wisconsin Oven Corp., East Troy, Wis., has shipped two direct gas-fired batch ovens with load capacity of 6000 pounds each to a leading automotive supplier for tempering tire molds to produce longer mold life.
Continue readingAluminum with added carbon nanotubes shows longer life under radiation
The Massachusetts Institute of Technology, Cambridge, reports its researchers have found that, at least in some nuclear reactors, adding less than 2% carbon nanotubes to aluminum can dramatically slow the breakdown process that causes it to become porous and brittle.
Continue readingCarbon nanotubes protect aluminum under radiation
Massachusetts Institute of Technology, Cambridge, reports that researchers have found that, at least in some nuclear reactors, adding less than 2% of carbon nanotubes to aluminum can dramatically slow the breakdown process that causes it to become porous and brittle.
Continue readingSpecialty stainless steel with 23% chromium provides higher corrosion resistance
Crompion International, Baton Rouge, La., reports that it has developed Cromgard C23, a specialty stainless steel with 23% chromium, 3.5 – 5% nickel, and 1 – 2% molybdenum.
Continue readingAlcoa awarded U.S. Army contract to reduce weight of combat vehicles
Alcoa, Pittsburgh, announces that it has been awarded a five-year contract from the U.S. Army worth up to $50 million for R&D projects focused on developing innovative lightweighting solutions for ground combat vehicles such as tanks.
Continue readingNorthrop Grumman selected to build B-21 stealth bomber
Northrop Grumman, Falls Church, Va., has released this artist’s rendering of its B-21 stealth bomber, selected last year by the United States Air Force as the Long Range Strike Bomber of the 21st century.
Continue readingLaser Gold Plating Technology Chosen for Plating the Oscar Statuettes
Epner Technology, Brooklyn, N.Y., was chosen to use its Laser Gold technology to electroplate gold onto the cast bronze Oscar statuettes this year. Laser Gold is a pure 24 kt gold that is also three times harder than ordinary pure gold.
Continue readingEuropean collaboration to build high-energy ball mill plant for nanopowders
The United Kingdom’s Centre for Process Innovation (CPI) and nine other European partners are collaborating in the design, scale-up, and build of a high energy ball-mill (HEBM) pilot plant for the production and validation of innovative nanostructured powders.
Continue readingArcam expands titanium powder production to 500 tons per year
Arcam AB, Sweden, has announced that its metal powder manufacturing subsidiary AP&C is significantly expanding its titanium powder production capacity with the commissioning of three new plasma atomizers.
Continue readingLaser gold plating technology coats Oscar statuettes
Epner Technology, Brooklyn, N.Y., was chosen to use its Laser Gold technology to electroplate gold onto the cast bronze Oscar statuettes this year.
Continue readingNIST ultrasound method detects cracks in capacitors
The National Institute of Standards and Technology, Gaithersburg, Md., and collaborators have demonstrated a nondestructive acoustic method for detecting cracks in ceramic capacitors before they go bad.
Continue reading3D-printed titanium hip implant features fully porous acetabular cup
Smith & Nephew, Andover, Mass., introduces its first 3D-printed titanium hip implant, the new Redapt revision acetabular fully porous cup with Conceloc technology.
Continue readingBonnell Aluminum to invest $18 million in extrusion line for auto structures
Bonnell Aluminum, Newnan, Ga., announces it will invest approximately $18 million over the next year to fund an expansion project that will include the purchase of a new state-of-the-art aluminum extrusion line at its Aacoa facility in Niles, Michigan.
Continue readingSolar Atmospheres partners with Pressure Technology for aircraft parts
Solar Atmospheres, Hermitage, Pa., announces that it now partners with Pressure Technology Inc. (PTI), Concord, Ohio, to provide heat treating of aircraft parts after they have been hot isostatically pressed to high density at the PTI facility.
Continue readingUTC Aerospace Systems opens $8 million advanced materials laboratory in Connecticut
UTC Aerospace Systems, Windsor Locks, Conn., has opened an $8 million, 20,000 ft2 state-of-the-art Materials and Process Engineering laboratory to support research, engineering, and production of advanced materials for aerospace applications.
Continue readingHelios G4 HX designed for advanced semiconductor failure analysis labs
FEI Co., Hillsboro, Oregon, announces that the new Helios G4 HX utilizes a patented inverted TEM sample preparation method to create high-quality lamellas for the most advanced semiconductor nodes.
Continue readingOlympus LED-illuminated microscope plus image analysis software simplify workflow
Olympus Corp., Tokyo, introduces the Olympus BX53M system microscope and Olympus Stream 2.1 image analysis software that together simplify workflow from observation to measurement, analysis, and reporting.
Continue readingAluminum alloy with high recycled content integrated into automotive structures
Novelis, Atlanta, announces that its RC5754 alloy, a new automotive product designed to contain up to 75% recycled aluminum content, has been successfully integrated into the structural components of high-volume production passenger vehicles.
Continue readingAlcoa to supply aluminum, aluminum-lithium, and titanium parts to Boeing
Alcoa, Pittsburgh, announces a long-term supply agreement with Boeing for multi-material aerospace parts for the 777X, Boeing’s newest commercial airplane; the 737 MAX, scheduled for first delivery in 2017; and the 787 Dreamliner.
Continue readingTimkenSteel develops faster process for manufacturing high-pressure tubing
TimkenSteel, Canton, Ohio, reports that it has developed a new process to manufacture high-pressure special bar quality tubing for the production of low-density polyethylene.
Continue readingMetalMaster furnace processes catalytic converter parts for a variety of industries
Ipsen, Cherry Valley, Ill., recently shipped a horizontal-loading MetalMaster vacuum furnace with two-bar gas quenching to a company in the Southwest United States for processing catalytic converter products, which are then used by such industries as aerospace, automotive and power generation.
Continue readingBodycote breaks ground for aluminum solution treatment furnace in California
Bodycote, England, held a ground breaking ceremony in February for a new aluminum solution treatment capability at its location in Westminster, California.
Continue readingRegistration opens for aerospace materials show
ASM International, Materials Park, Ohio, announces that early bird registration is open for the 27th AeroMat Conference and Exposition May 23-25 in Bellevue, Washington.
Continue readingSunEdison Semiconductor initiates agreements to assure polysilicon supply
SunEdison Semiconductor Ltd., says that over the past several months it has been working on several initiatives to improve contingency planning for polysilicon supply and to manage the transition to multiple sources.
Continue readingSunEdison Semiconductor initiates agreements to assure polysilicon supply
SunEdison Semiconductor Ltd., St. Peters, Mo., says that over the past several months it has been working on several initiatives to improve contingency planning for polysilicon supply and to manage the transition to multiple sources.