Spray Tips: Spray drying

Spray drying, a method that rapidly dries aqueous or solvent-based solutions or slurries to particulate form by atomizing the liquid in a heated chamber, can be used to agglomerate fine powders and is an important method for the dehydration of fluid foods, such as milk, coffee, and egg powder extensively used in the pharmaceutical and chemical industries.