Confluent Medical Technologies, Scottsdale, AZ, announced the release of Ultra Polyimide, a new high-performance polymer tubing that offers approximately double the strength of conventional polyimide. This innovation is aimed at enabling next-generation medical devices that demand both durability and miniaturization.
Ultra Polyimide addresses the need for thinner-walled tubing that maintains structural integrity, allowing for greater design flexibility and improved device performance. By preserving the inner lumen while reducing material usage, engineers can integrate additional features into delivery devices without compromising mechanical strength.
Jill Ellison, vice president of operations at Confluent’s High Precision Polymer Tubing Center of Excellence, noted that the material enables designers to maintain essential column and tensile strength, which opens up opportunities for innovation in minimally invasive technologies.
The tubing is also manufactured without the use of REACH- or EU MDR-restricted solvents, including NMP (n-Methyl-2-pyrrolidone), a substance identified by the U.S. Environmental Protection Agency as posing health risks in industrial settings. By eliminating NMP from the production process, Confluent supports regulatory compliance and enhances both workplace and patient safety.
Ultra Polyimide is now available with lead times of three to four weeks, offering a timely solution to the evolving needs of the medical device industry.