Heat treating an anvil sleeve in a molten salt quenching bath Published by Video descriptionThis video from Alcon Tool shows the process of heat treating an anvil sleeve in a salt quench bath. Published:December 5, 2022 Related videos How a metal with a memory will shape our future on Mars How to make a lava lamp Seven planets orbit Trappist-1 dwarf star 40 light years away