Development of a Residual Stress Standard

In the past ten to fifteen years, significant progress toward the understanding and management of residual stresses in metallic structure has been made under the auspices of numerous Metals Affordability Initiative (MAI) projects, Small Business Innovative Research (SBIR) projects, USAF program funded projects, and many others. In January 2020, the ASM International Technical Committee on Residual Stress formed a subcommittee on residual stress standards development, whose goal is to promote the development of standards and specifications for the measurement, modeling, understanding and management of residual stress

Continue reading

One Minute Mentor: Effect of porosity on the heat treatment of powder metallurgy steels

Porosity has the greatest single effect on the response of PM Steels to heat treatment compared with conventional steels. The majority of parts have a porosity between 5 and 15 vol%, far more than is found in a typical casting. Every mechanism in press and sinter is subject to diminishing returns; i.e., compact density has a decreasing dependence on compaction pressure, as does sintering and homogenization.

Continue reading

One Minute Mentor: Sintering of power particles

During sintering, metallurgical bonds form between powder particles. Strength, ductility, toughness, and electrical and thermal conductivities increase with increasing density. If different materials were blended together, interdiffusion could promote the formation of alloys and intermetallic phases. As a consequence of the density increases, size decreases.

Continue reading

Seco/Warwick introduces Zeroflow

Seco/Warwick, Poland, has introduced a new gas nitriding technology called ZeroFlow to the global industry in cooperation with scientists from the Poznan University of Technology. ZeroFlow reduces process costs while providing more ecologically friendly performance.

Continue reading

NanoAL brings Addalloy to Mitsubishi

NanoAL LLC, Boston, has signed a commercial license agreement with Mitsubishi Corp. RtM Japan Ltd. to bring its Addalloy family of advanced aluminum alloy powders to the metal additive manufacturing market in Asia.