A significant practical advantage of the CA-6NM stainless steel casting alloy is its relative freedom from the rapid drop in hardness when tempered above about 950°F.  The graph shows clearly that a given increase in tempering temperature produces a much more gradual decrease in hardness than with CA-15. This makes heat treating much easier and cheaper, and decreases the frequency of rejections and/or the necessity for reheat treatment.