Oerlikon Group, Switzerland, announces the successful closing of the transaction to acquire Metco from Sulzer AG ahead of schedule.
RTI acquires Dynamet for its advanced titanium powder metal technology
RTI International Metals Inc., Pittsburgh, has acquired Dynamet Technology Inc., an industry innovator in titanium powder metallurgy and a supplier of near-net shape titanium and titanium alloy preforms and components to commercial aerospace, defense, biomedical and industrial customers.
Al-Fe Wadsworth receives Nadcap accreditation for glycol quenching
Al-Fe Heat Treating, Fort Wayne, Ind., has added glycol quenching to its list of Nadcap-accredited aluminum heat treat services at its plant in Wadsworth, Ohio.
Selective laser melting to produce aerospace components
Fraunhofer Institute for Laser Technology IPT, Germany, is developing Selective Laser Melting technology to build aerospace components via additive manufacturing.
Nikon 750kV microfocus X-ray source enables NDT inspection of steel parts
Nikon Metrology Inc., Brighton, Mich., announces a unique 750 kV x-ray source with micron level spot size.