Alcoa, Pittsburgh, has broken ground on a new state-of-the-art, $100 million, 320,000-square-foot facility in La Porte, Indiana, where it will produce nickel-base superalloy jet engine parts.
Ipsen ships 15 vacuum furnaces for aerospace, automotive, and energy industries
Ipsen, Cherry Valley, Ill., has recently shipped more than 15 vacuum furnaces to customers around the world for a diverse range of applications and industries.
VPC and Liquidmetal sign agreement to grow amorphous metal technology
Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., announces that it has signed an amended sublicense agreement with Visser Precision Cast LLC (VPC) in which Liquidmetal is freed from its commitment to use VPC as its exclusive contract manufacturer, and VPC is freed from its commitment to use Liquidmetal as its exclusive sales and R&D channel.
Ford heat treatment nearly doubles strength of aluminum parts in Ford F-150
Ford Motor Co., Dearborn, Mich., says that the aluminum door panels and box panels in its new Ford F-150 pickup truck are more resistant to dents than the previous steel panels.
Solar Atmospheres certified for liquid penetrant inspection testing
Solar Atmospheres, Hermitage, Pa., has been certified by Nadcap for fluorescent liquid penetrant inspection.