Seco Warwick, Meadville, Pa., introduces its Super IQ integral quench furnace and UCM 4D Quench system.
Solar Atmospheres 14-foot car-bottom air furnace can treat loads up to 30,000 pounds
Solar Atmospheres of Western PA, Hermitage, recently installed a 14-foot long car bottom air furnace for the tempering of large tool steel components, as well as the age hardening processes of nickel-based alloys and precipitation hardenable stainless steels.
One Minute Mentor: Martensitic heat treating
The graph shows the tempering response of hardened 52100 bearing steel.
Arcast produces titanium powder with zero risk of ceramic/oxide contamination
Arcast Inc., Oxford, Maine, reports that it has successfully produced a titanium superalloy powder with an as-atomized D50 of 20 µm, with narrow size distribution and with little-to-no oxygen pickup.
ITSC 2019 presentation: Solid-State Additive Manufacturing
Inovati, Santa Barbara, Calif., presented a discussion about the application of its impact consolidation Kinetic Metallization (KM) process to an advanced and superior 3D manufacturing technology.