Carbon infused with zirconium, boron, and titanium can withstand heat of hypersonic flight

Researchers from the University of Manchester in England, and Central South University in China, announce that they have developed a carbide coating in which powders of zirconium, boron, and titanium are infused into a carbon composite, producing a coating that can withstand the high temperatures of aircraft structures flying at over five times the speed of sound.