Lindberg MPH, Riverside, Mich., reports that its Treet-All light industrial box furnace is suited for multiple applications, including annealing, ashing, austempering, brazing, preheating, and solution treating.
Bodycote plans to build new facility in Illinois for advanced heat treating technologies
Bodycote, U.K., the world’s largest provider of heat treatment and specialist thermal processing services, announces plans to open a new heat treating facility by late 2019 in Elgin, Illinois.
Department of Energy to award $38 million for projects to advance coal-fired power plants
The U.S. Department of Energy, Washington, announces up to $38 million in federal funding for cost-shared R&D projects enhancing technologies that improve the overall performance, reliability, and flexibility of the nation’s existing coal-fired power plant fleet.
Supersonic Spray repairs 1937 vintage aluminum oil pan with its cold spray technology
Supersonic Spray Technologies, a division of Centerline, Windsor, Ontario, announces that its engineers have restored an aluminum casting oil pan on a 1937 Alfa Romeo 8C 2900B Touring Berlinetta with its cold spray technology.
Titanium carbide nanoparticles infused into aluminum alloy 7075 enable strong welds
Engineers at the UCLA Samueli School of Engineering announce that they have developed a way to weld aluminum alloy AA 7075 by infusing titanium carbide nanoparticles into welding wires, which results in welded joints with a tensile strength up to 392 MPa.