Seco Vacuum, Meadville, Pa., reports that a growing American manufacturer has recently ordered a new precision gas nitriding furnace with ZeroFlow.
Wisconsin Oven ships belt conveyor oven for preheating aluminum forging billets
Wisconsin Oven Corp., East Troy, has shipped a forging company a natural gas-fired conveyor oven that will serve as a preheating oven for aluminum billets.
Instron “Errors in Your Data” online course helps operators identify data integrity issues
Instron, Norwood, Mass., launches an all-new online training course designed to help operators of materials testing systems understand data integrity issues they may encounter during testing.
Goodfellow to offer Victrex mineral-filled semicrystalline and amorphous PEEK film
Goodfellow, Coraopolis, Pa., announces a major expansion of its range of polyetheretherketone (PEEK) materials to include 12 different forms: film, sheet, fiber, monofilament, powder, granule, tube, rod, mesh, bolt, nut, and washer.
One-Minute Mentor: Heat Treating and Properties of Ductile Iron
The basic structural differences between the ferritic and austenitic classes are shown in the continuous cooling transformation (CCT) diagram and cooling curves for furnace cooling, air cooling, and quenching.