Molten aluminum poured over 3D-printed steel lattice multiplies damage tolerance
Oak Ridge National Laboratory, Tenn., and Rice University, Houston, report that a new manufacturing method developed by Oak Ridge and Rice combines 3D printing with traditional casting to produce damage-tolerant components composed of multiple materials.
ATI and GE Aviation joint venture to develop titanium alloy powder for 3D printing
Allegheny Technologies Inc., Pittsburgh, and GE Aviation, Cincinnati, announce a joint venture for the development of a new manufacturing technology for meltless titanium alloy powder.
One Minute Mentor: Nitrogen-Expanded Austenite
The graph shows hardness-depth profiles of nitrided AISI 316. A profile for carburizing is shown for comparison.
Featured Paper from Heat Treat 2017
Today’s competitive environment often requires one to do more with less – to make equipment last longer and run more efficiently.