I would like to dedicate the TSS President’s Message to two outstanding individuals who were recently selected for induction into the ASM Thermal Spray Society Hall of Fame (HoF). This honor was established in 1993 to recognize outstanding leaders who have made significant achievements and contributions to the science, technology, practice, education, management, and advancement of thermal spraying.
Spray Tips: What is a Splat?
Splat is the term given to a single impacted droplet/particle, as illustrated in the diagram. Many overlapping splats solidify and adhere to one another to form a continuous coating layer. Thus, the splat is the basic structural building block in thermal spray coatings.
Carpenter buys Puris for its titanium powder capabilities
Carpenter Technology Corp., Philadelphia, announces that it has agreed to purchase substantially all of the assets and business of Puris LLC, a producer of titanium powder for additive manufacturing and advanced technology applications.
Steel Dynamics invests $28 million to expand rolling capacity at its Roanoke facility
Steel Dynamics, Fort Wayne, Ind., recently invested $28 million for a reheating furnace and a new finishing area in its Roanoke Bar Division to increase rolling capacity from the current 500,000 tons to over 600,000 tons per year.