The International Titanium Association, Northglenn, Colo., announces that the Titanium 2016 conference and exhibition will focus on the global titanium industry.
Bodycote Ipswich heat treating facility earns MedAccred status
Bodycote, England, announces that its facility in Ipswich, Mass., has earned MedAccred accreditation, underlining its high standards of quality.
One Minute Mentor: Stress Relieving Type 347 Stainless Steel
Although stabilized alloys do not require high-temperature annealing to avoid intergranular corrosion, the stress-relieving temperature exerts an influence on the general corrosion resistance of these alloys.
Fluorescent microcapsules identify microscopic failure
The Autonomous Materials Systems Group at the Beckman Institute for Advanced Science and Technology, Urbana, Ill., recently devised a way to identify microscopic damage in polymers and composites by incorporating microcapsules containing materials that fluoresce under stress.
ElectroForce 3310 provides fatigue test controllability for high and low forces
TA Instruments, New Castle, Del., announces that the ElectroForce 3310, the newest addition to the TA Instruments ElectroForce load frame family, delivers 1 kN of force capacity with 25 mm of dynamic displacement.