Missouri S&T developing high-strength TRIP steel for autos

Missouri University of Science and Technology, Rolla, announces that a third-generation high-strength steel being developed by Missouri S&T metallurgical engineers should be lighter and easier to make, while being strong enough to address automotive safety concerns.