Carbon control during sintering improves quality of MIM parts

Linde North America Inc., Murray Hill, N.J., and Megamet Solid Metals, Earth City, Mo., a custom metal-injection molding company, have shown that the quality of metal-injection-molded parts could be significantly enhanced by following Linde’s advanced Sinterflex atmosphere control system.