Nanovea, Irvine, Calif., announces the M3 hardness tester with automated indentation technology.
Hi-Tek Manufacturing receives Nadcap accreditation for heat treating and more
Hi-Tek Manufacturing, Mason, Ohio, which serves the gas turbine industry, announces that it has received Nadcap accreditation for heat treating and for brazing, hardness testing for heat treating, and pyrometry capabilities.
Mitsubishi and Siemens start joint venture Primetals Technologies operations
Solar Atmospheres heat treats titanium manifold for Orion spacecraft
Solar Atmospheres of Western Pennsylvania, Hermitage, Pa., announces that it vacuum heat-treated the titanium manifold in the Launch Abort System of the NASA Orion spacecraft launched in December.
Ajax Tocco temper ovens heat treat automotive constant-velocity joints
Ajax Tocco Magnethermic Corp., Warren, Ohio, has supplied three temper ovens to a major automotive parts manufacturer in Mexico for the tempering of constant-velocity joints.