Mass-flow-controlled UHP/HVOF system cuts costs by up to 25%

Flame Spray Technologies, The Netherlands, has introduced a state-of-the-art mass flow controlled UHP/HVOF eGun coating system that reportedly enables cost reductions up to as much as 25% compared with conventional liquid-fuel HVOF systems.