ASB upgrades its Impact Innovations cold spray system

ASB Industries, Barberton, Ohio, announces that it has upgraded its current Impact Innovations high-pressure cold spray equipment to the most advanced system, which allows a wider variety of material spraying capabilities using nitrogen as the main process gas.