Alcoa, Pittsburgh, announced at the Farnborough Air Show that it has signed a ten-year, $1.1 billion agreement with Pratt & Whitney for state-of-the-art jet-engine components.
Alcoa’s aluminum bonding technology wins R&D 100 award
Alcoa, Pittsburgh, announces that R&D Magazine has named Alcoa 951 — an enabler for adhesive bonding of aluminum-intensive vehicles (AIVs) — an R&D 100 Award winner.
Notre Dame and General Electric to collaborate on gas turbine R&D facility
The University of Notre Dame, South Bend, Ind., and General Electric Power & Water, Schenectady, N.Y., announce plans to work together to build a $36 million research and test facility with the goal of making better massive gas turbines used by aircraft, power plants, and the oil and gas industry.
Alcoa to acquire Firth Rixson for its aerospace forging capabilities
Alcoa, Pittsburgh, has signed a definitive agreement to acquire Firth Rixson, a global leader in aerospace jet engine components, from Oak Hill Capital Partners, for $2.85 billion in cash and stock.
AFC-Holcroft batch furnace customized for Specialty Steel Treating
AFC-Holcroft, Wixom, Mich., announces that Specialty Steel Treating is adding a new Universal Batch Quench integral quench furnace to its facility in Fraser, Mich.