One Minute Mentor: Nitriding

Powder metallurgy parts can be nitrided using alkali salts, gases, and plasmas, with the majority of applications using gases. Alkali salts can be used in some applications, because trapped salts may not be detrimental if the part is constantly immersed in oil during service.