Constellium developing aluminum-lithium alloys for NASA

Constellium, Paris, is developing an aluminum-lithium alloy solution, Airware®, that will be used for NASA’s Launch System rocket and Orion spacecraft, for missions that will ultimately send humans farther into deep space than ever before. Airware’s inherent low density, high-specific stiffness, strength and excellent mechanical properties provide the high-performance characteristics required during the demanding launch and landing phases.

Ipsen’s new PdMetrics feature offers additional diagnostics

Ipsen, Cherry Valley, Illinois launched new features on its PdMetrics dashboard that monitors incoming three-phase utilities, voltage, and frequency on Ipsen’s Titan 2.0 vacuum furnaces. This addition offers further diagnostics for the diffusion pump heater assembly.