Researchers use neutrons to study weld-induced stress relief in energy applications

The U.S. Department of Energy has a team of researchers exploring how a weld is put together atom by atom in order to unlock the key to making crack-free welds. The goal is to investigate the performance of welds used to build large thermal energy storage tanks at concentrating solar plants—facilities with vast networks of mirrors used to collect solar energy, some stretching several million square feet in size.

Nitrex supplies Alugen Aluminum with nitriding system

Nitrex Metal Inc., Montreal, has supplied the Turkish aluminum extrusion company, Alugen Aluminium, with a high-performance compact nitriding/nitrocarburizing system allowing the company to bring all manufacturing operations in-house for more optimal work planning and quality control. Founded in 2012, Alugen is a dynamic company and the only business of its kind in Turkey operating in a free trade zone, with customers in various European countries.

Steel Authority of India issues final acceptance certificate to CAN-ENG furnaces

CAN-ENG Furnaces International LTD has been issued the Final Acceptance Certificate (FAC) for the Roller Hearth Plate Quench and Temper system by the Steel Authority of India Limited (SAIL). The system is designed to heat treat a wide range of plates from 6 mm to 100 mm thickness x 3,000 mm wide and lengths up to 13,000 mm long in a wide variety of grades for commercial and non-commercial applications.

ECM Technologies launches new ECO furnace

ECM Technologies, Grenoble, France announced the release of a new furnace system that will replace current sealed quench (SQ) or integral quench (IQ) style furnaces. The system offers a cleaner, safer and greater performance in comparison to traditional SQ or IQ furnace on the market today.