What’s New
-
The 2019 HTS-Bodycote Best Paper in Heat Treating, “Rapid Tempering: Opportunities and Challenges” by Virginia Judge Euser, Los Alamos National Laboratory and Colorado School of Mines, has been published in the July issue of Journal of Materials Engineering and Performance. Euser’s co-advisors were A.J. Clarke and J.G. Speer, Colorado School of Mines. Read more>
-
Vol. 4E, available for purchase, completes the HT Handbook set