Lindberg ships full muffle mesh belt conveyor furnace to manufacturing industry

September 19, 2023
Source: ASM International

Lindberg/MPH, Mich,  a leading manufacturer of heat treat furnaces, announced the shipment of a continuous full muffle mesh belt conveyor furnace to an industrial manufacturer.

This conveyor furnace is designed for applications with a nitrogen atmosphere and a maximum temperature of 1,100°C. Additionally, the furnace has a hydrogen flow meter and combustible gas system so the customer can run a hydrogen atmosphere when needed. The combustible gas system provides a timed nitrogen gas purge of the muffle before process gas can be introduced into the furnace muffle. The conveyor furnace has overall dimensions of 128” L x 22” W 41.5” H. There are tables at both ends of the furnace for loading and unloading of the product. The unit is designed with four (4) temperature zones and a water-cooling section that parts travel through prior to exiting the chamber.