Magnesium alloy designed for down-hole oil and gas fracking tools dissolves after use

February 15, 2016
Source:

Magnesium Elektron, England, introduces SoluMag, a proprietary high-strength, soluble magnesium alloy developed specifically for making down-hole oil and gas industry fracking tools that quickly and safely dissolve after use. The company has applied for a patent for the alloy.

Traditional fracking requires expensive machinery to remove plugs, balls, and other temporary tools that have served their purpose, to enable an unimpeded flow of oil and gas. Tools made from SoluMag dissolve completely after use, eliminating the need for such costly intervention.

"SoluMag dissolves quickly, predictably, and at lower temperatures than other soluble materials used in these applications," said Guy Roberts, head of sales and marketing for Magnesium Elektron. The first public showing of SoluMag took place at the Global Petroleum Show in Calgary, Canada, in June 2015. A time-lapse video showed the material being dissolved in a saline solution. Also shown were samples at various levels of dissolution, as well as test data covering strength and corrosion rates. This generated a high level of interest from completion companies and tool suppliers and led to initial product sales for laboratory and field testing.

Magnesium Elektron has since announced further product developments, including the ability to customize rates at which the alloy dissolves.

Mr. Roberts noted that SoluMag joins a long line of highly specialized magnesium alloys developed by Magnesium Elektron, including SynerMag, a dissolving alloy now undergoing in-body tests for cardiovascular stents. "Our aerospace pedigree means that our alloys are of the highest quality and consistency, so end-users can be confident that tools made from SoluMag will behave predictably down-hole."

www.magnesium-elektron.com

 

Magnesium alloy designed for down-hole oil and gas fracking tools dissolves after use

Magnesium Elektron, England, introduces SoluMag, a proprietary high-strength, soluble magnesium alloy developed specifically for making down-hole oil and gas industry fracking tools that quickly and safely dissolve after use.

Continue reading

Bodycote opens new plants in Georgia and South Carolina

January 12, 2016
Source:

Bodycote, U.K., announces two new heat treatment plants in the southeastern United States: Covington, Ga., and Greenville, S.C.  The Covington plant will open in Spring 2016 to replace the nearby Conyers facility. Primarily serving automotive and general industrial customers, the new plant will be more than double the size of the existing Conyers facility, immediately increasing capacity to serve the Georgia and Florida marketplaces. 

The Greenville plant is a new Nadcap-accredited facility that will serve the region's aerospace manufacturing supply chains. It is scheduled to be operational mid-2016 and provides further expansion opportunities to install additional key services in response to customer demand.

These new facilities are part of Bodycote's investment and expanded services strategy to serve the diverse range of industries in the Southeast United States.

Through heat treatment, metal joining, surface technology, and hot isostatic pressing, Bodycote improves the properties of metals and alloys, extending the life of vital components for a wide range of industries, including aerospace, defense, automotive, power generation, oil & gas, construction, medical and transportation.

www.bodycote.com

 

Bodycote opens new plants in Georgia and South Carolina

Bodycote, U.K., announces two new heat treatment plants in the southeastern United States: Covington, Ga., and Greenville, S.C.

Continue reading

Metal powders are potential replacement for fossil fuels

December 17, 2015
Source:

Can you imagine a future where your car is fueled by iron powder instead of gasoline? Metal powders, produced using clean primary energy sources, could provide a more viable long-term replacement for fossil fuels than other widely discussed alternatives, such as hydrogen, biofuels or batteries, according to a study researchers at McGill University, Canada.

"Technologies to generate clean electricity—primarily solar and wind power—are being developed rapidly; but we can't use that electricity for many of the things that oil and gas are used for today, such as transportation and global energy trade," says Professor Jeffrey Bergthorson.

"Biofuels can be part of the solution, but won't be able to satisfy all the demand; hydrogen requires big, heavy fuel tanks and is explosive, and batteries are too bulky and don't store enough energy for many applications," says Bergthorson. "Using metal powders as recyclable fuels that store clean primary energy for later use is a very promising alternative solution."

Novel concept

The research includes other McGill researchers and a European Space Agency scientist in the Netherlands, lays out a novel concept for using tiny metal particles—similar in size to fine flour or icing sugar—to power external-combustion engines.

Unlike the internal-combustion engines used in gasoline-powered cars, external-combustion engines use heat from an outside source to drive an engine. External-combustion engines, modern versions of the coal-fired steam locomotives that drove the industrial era, are widely used to generate power from nuclear, coal or biomass fuels in power stations.

The idea of burning metal powders is nothing new – they've been used for centuries in fireworks, for instance. Since the mid-20th century, they've also been used in rocket propellants, such as the space shuttle's solid-fuel booster rockets. But relatively little research has been done in recent decades on the properties of metal flames, and the potential for metal powders to be used as a recyclable fuel in a wide range of applications has been largely overlooked by scientists.

Recyclable after combustion

The idea put forward by the McGill team takes advantage of an important property of metal powders: when burned, they react with air to form stable, nontoxic solid-oxide products that can be collected relatively easily for recycling – unlike the CO2 emissions from burning fossil fuels that escape into the atmosphere.

Using a custom-built burner, the team demonstrated that a flame can be stabilized in a flow of tiny metal particles suspended in air. Flames from metal powders "appear quite similar" to those produced by burning hydrocarbon fuels, according to researchers. "The energy and power densities of the proposed metal-fueled heat engines are predicted to be close to current fossil-fueled internal combustion engines, making them an attractive technology for a future low-carbon society."

Iron could be the primary candidate for this purpose. Millions of tons of iron powders are already produced annually for the metallurgy, chemical and electronic industries. And iron is readily recyclable with well-established technologies, and some novel techniques can avoid the carbon dioxide emissions associated with traditional iron production using coal.

Next step: building a prototype

While laboratory work at McGill and elsewhere has shown that the use of metal fuels with heat engines is technically feasible, no one has yet demonstrated the idea in practice. The next step toward turning the lab findings into usable technology, therefore, will be "to build a prototype burner and couple it to a heat engine," Bergthorson says. "Developing metal recycling processes that don't involve CO2 emissions is also critical."

David Jarvis, head of strategic and emerging technologies at the European Space Agency, adds: "We are very interested in this technology because it opens the door to new propulsion systems that can be used in space and on earth. The shift away from fossil fuels for vehicle propulsion is a clear trend for the future. While not perfected and commercialized today, the use of low-cost metallic fuels, like iron powder, is a worthy alternative to petrol and diesel fuels. If we can demonstrate, for the first time, an iron-fueled engine with almost zero CO2 emissions, we believe this would then trigger even more innovation and cost reduction in the near future."

Research on metal combustion at McGill has been funded over the past 20 years by the Natural Sciences and Engineering Research Council of Canada, the Canadian Department of National Defence, the U.S. Defense Threat Reduction Agency, the Canadian Space Agency, the European Space Agency, Martec Ltd. (Halifax, NS), and the Trottier Institute for Sustainability in Engineering and Design.

Image caption — Stabilized flames of different metal powders burning with air, compared to a methane-air flame.

Metal powders are potential replacement for fossil fuels

Can you imagine a future where your car is fueled by iron powder instead of gasoline?

Continue reading

Berkshire Hathaway to acquire Precision Castparts in cash transaction

August 12, 2015
Source:

The boards of directors of Berkshire Hathaway Inc., Omaha, Neb., and Precision Castparts Corp., Portland, Ore., have unanimously approved a definitive agreement for Berkshire Hathaway to acquire all outstanding PCC shares for $235 per share in cash. PCC will remain headquartered in Portland as a wholly owned subsidiary of Berkshire Hathaway, and will continue to do business around the world under the Precision Castparts name. The transaction is valued at approximately $37.2 billion, including outstanding PCC net debt.

"I've admired PCC's operation for a long time," says Warren E. Buffett, Berkshire Hathaway chairman and chief executive officer. "For good reasons, it is the supplier of choice for the world's aerospace industry, one of the largest sources of American exports. Berkshire's Board of Directors is proud that PCC will be joining Berkshire."

"We are very pleased to be joining forces with Berkshire Hathaway," says Mark Donegan, PCC's chairman and chief executive officer. "We see a unique alignment between Warren's management and investment philosophy and how we manage PCC for the long-term.

"We believe that as part of Berkshire Hathaway, PCC will be exceptionally well-positioned to support our customers into the future. This transaction offers compelling and immediate value for our shareholders, and allows PCC's employees to continue to operate in the same manner that has generated many years of exceptional service and performance."

The transaction requires approval by a majority of PCC's outstanding shares. Closing is expected during the first quarter of calendar 2016, subject to customary closing conditions, including clearance under the Hart-Scott-Rodino Act and competition clearance in certain foreign jurisdictions.

Precision Castparts Corp. is a worldwide, diversified manufacturer of complex metal components and products. It serves the aerospace, power, and general industrial markets. PCC is a market leader in manufacturing complex structural investment castings and forged components for aerospace markets, machined airframe components, and highly engineered, critical fasteners for aerospace applications, and in manufacturing airfoil castings for the aerospace and industrial gas turbine markets. PCC also is a leading producer of titanium and nickel superalloy melted and mill products for the aerospace, chemical processing, oil and gas, and pollution control industries, and manufactures extruded seamless pipe, fittings, and forgings for power generation and oil and gas applications.

www.berkshirehathaway.com

http://www.precast.com/investors/press_release/?id=666

 

 

Berkshire Hathaway to acquire Precision Castparts in cash transaction

The boards of directors of Berkshire Hathaway Inc., Omaha, Neb., and Precision Castparts Corp., Portland, Ore., have unanimously approved a definitive agreement for Berkshire Hathaway to acquire all outstanding PCC shares for $235 per share in cash.

Continue reading

Bodycote expands operations in Houston

May 15, 2015
Source:

Bodycote, U.K., announces that it will expand its services at its two locations in Houston. In the third quarter, new offerings in north Houston will include nitriding, vacuum heat treatment, and vacuum brazing, to provide customers with comprehensive and efficient services from a single facility. Bodycote is also investing in more capacity at its second Houston location.

Together, these enhancements ensure that Bodycote's customers experience better service, superior quality and faster turnaround time. The company continues to play a vital role in the area's oil & gas, power generation and general industrial supply chains.

With more than 180 accredited facilities in 26 countries, Bodycote is the world's largest provider of thermal processing services. Through heat treatment, metal joining, surface technology, and Hot Isostatic Pressing (HIP), Bodycote improves the properties of metals and alloys, extending the life of vital components for a wide range of industries, including aerospace, defense, automotive, power generation, oil & gas, construction, medical, and transportation. 

www.bodycote.com

 

Bodycote expands operations in Houston

Bodycote, U.K., announces that it will expand its services at its two locations in Houston.

Continue reading

SSAB launches Strenx brand for high-strength steels

April 22, 2015
Source:

SSAB, Stockholm, has launched Strenx, a new high-strength structural steel product brand that includes Optim, Weldox, and Domex steels that are well-known trademarks of SSAB and the former Ruukki. Strenx is well-suited for agriculture, the frames of heavy mobile machines, rolling stock, offshore, and construction sectors.

Strenx features the world's widest choice of high-strength structural steels, in terms of both strength and dimensional range. Yield strengths range from 600 MPa to 1300 MPa, which is the strongest steel available on the market. Strenx is available in plate, strip and tubular products in thicknesses ranging from 0.7 mm to 160 mm.

Strenx is designed for sectors where structural strength and weight savings are key competitive factors, especially in the lifting, handling, and transportation industry. Now customers will be able to design more competitive and sustainable products – cranes that reach farther, trailers that carry more payload, trucks that use less fuel.

"Strenx embodies over 50 years of experience in high-strength steels," says Gregoire Parenty, Head of Market Development at SSAB. "We give full support to designers and customers to help them upgrade to Strenx. By sharing our in-depth experience and wide knowledge of steel we can guarantee the best results for end-product performance."

Strenx comes with guaranteed product consistency, services to help customers, and permanent assistance to enhance end-product performance.

www.strenx.com

 

SSAB launches Strenx brand for high-strength steels

SSAB, Stockholm, has launched Strenx, a new high-strength structural steel product brand that includes Optim, Weldox, and Domex steels that are well-known trademarks of SSAB and the former Ruukki.

Continue reading

Ipsen provides range of atmosphere furnaces for North American market

February 25, 2015
Source:

Ipsen, Cherry Valley, Ill., reports that since 2010, the company has successfully installed more than 50 atmosphere furnaces, as well as temper and auxiliary equipment throughout North America. Atmosphere furnaces provide the flexibility to carburize, nitride, and harden a wide range of parts with different materials, case depths, hardenability, and geometries.

These installations include single- and double-chamber sealed quench, vertical retort, pusher, and box furnaces. For example, Ipsen pusher furnaces drive parts through the full carburizing and nitriding processes, including preheating, washing, tempering and cooling, all in a fully-automated, "lights-out" system with customized layouts.

Ipsen has one of the largest installed bases of atmosphere furnaces in the United States – several thousand since its founding in 1948.  – Ipsen continues to deliver atmosphere solutions that meet a range of customer needs. These installations were designed for a range of applications and industries – automotive, aerospace, commercial, and energy.

For Ipsen, a key part of innovating is listening to the specific needs and challenges of their customers and then providing ideal solutions that meet those needs. As companies are faced with constantly evolving requirements and processes, nothing is more essential than finding heat-treating equipment that provides the necessary solutions.

www.IpsenUSA.com/Atmosphere. 

 

Ipsen provides range of atmosphere furnaces for North American market

Ipsen, Cherry Valley, Ill., reports that since 2010, the company has successfully installed more than 50 atmosphere furnaces, as well as temper and auxiliary equipment throughout North America.

Continue reading

ATI to supply nickel-base alloy plate for a pipeline project

November 26, 2014
Source:

Allegheny Technologies Inc., Pittsburgh, has received an additional order for its nickel-base alloy plate for a large oil and gas pipeline project. ATI previously announced that it had booked initial orders for this project. Shipments are scheduled to begin in late fourth quarter 2014 and continue through the first half of 2015.

"Total expected revenue of approximately $145 million from these orders represents the largest participation in a project in ATI's history," said Rich Harshman, Chairman, President and Chief Executive Officer. "For perspective, expected revenue from these orders is greater than 25% of ATI's sales to the Oil & Gas/Chemical Process Industry for the first nine months of 2014. We received a large share of this project due to the quality of our nickel-based alloy plate that is enabled by ATI's unique supply chain, including our Flat Rolled Products segment specialty alloy plate facility."

www.ATImetals.com

 

ATI to supply nickel-base alloy plate for a pipeline project

Allegheny Technologies Inc., Pittsburgh, has received an additional order for its nickel-base alloy plate for a large oil and gas pipeline project.

Continue reading