Featured Paper from Heat Treat 2017

July 7, 2017
Source:

Mr. Pete Kerbel , Ipsen USA, Cherry Valley, IL

Today's competitive environment often requires one to do more with less – to make equipment last longer and run more efficiently. As such, there are several factors that go into making your equipment run to the best of its ability. With our industry becoming more demanding, there has never been a better time to ask the question:  "Where, and in what, do I invest my money with aging equipment?"

This paper offers a close-up look at what is possible when weighing different options for upgrading an aging vacuum furnace, focusing on the many factors that go into choosing the right upgrades and repairs for both your equipment and process requirements.

Specific topics covered include:

  • The three factors you should always consider before replacing a hot zone
  • What is required for data acquisition?
  • The role preventative maintenance plays in extending your equipment's life span
  • How much is too much to invest in aging equipment?

View Abstract

Featured Paper from Heat Treat 2017

Today’s competitive environment often requires one to do more with less – to make equipment last longer and run more efficiently.

Continue reading

NIST awards $12 million to MEP centers in 11 states to support manufacturers

January 15, 2017
Source:

The National Institute of Standards and Technology, Gaithersburg, Md., announces that its Hollings Manufacturing Extension Partnership (MEP) program has awarded a total of nearly $12 million in first-year funding to 11 organizations that will operate MEP centers in Delaware, Hawaii, Iowa, Kansas, Maine, Mississippi, Nevada, New Mexico, North Dakota, South Carolina, and Wyoming.

MEP centers in all 50 states and Puerto Rico support small and medium-size manufacturers and are dedicated to enhancing the productivity and technological performance of U.S. manufacturing. The agreements have five-year periods of performance that begin April 1, 2017, and they will provide nearly $60 million in total funding during that time.

The following organizations will sign cooperative agreements to operate MEP centers:

Delaware Technical Community College (Newark) - $500,000

High Technology Development Corporation (Honolulu, Hawaii) - $500,000

Iowa State University of Science & Technology (Ames) - $1,859,206

Mid-America Manufacturing Technology Center (Overland Park, Kansas) - $1,864,950

Maine Manufacturing Extension Partnership (Augusta) - $863,522

Mississippi Manufacturers Association (Jackson) - $1,003,782

Board of Regents, Nevada System of Higher Education, University of Nevada-Reno - $756,001

New Mexico Manufacturing Extension Partnership (Albuquerque) - $1,360,802

The Dakota Manufacturing Extension Partnership Inc. (Bismarck, North Dakota) - $500,000

South Carolina Manufacturing Extension Partnership (Columbia) - $2,268,003

University of Wyoming (Laramie) - $500,000

 

 

 

 

 

https://www.nist.gov/mep

 

NIST awards $12 million to MEP centers in 11 states to support manufacturers

The National Institute of Standards and Technology, Gaithersburg, Md., announces that its Hollings Manufacturing Extension Partnership (MEP) program has awarded a total of nearly $12 million in first-year funding to 11 organizations that will operate MEP centers in Delaware, Hawaii, Iowa, Kansas, Maine, Mississippi, Nevada, New Mexico, North Dakota, South Carolina, and Wyoming.

Continue reading

ASM Appoints New Managing Director

September 13, 2016
Source: ASM International

ASM Appoints New Managing Director

The ASM International Board of Trustees announces the appointment of William T. (Bill) Mahoney as Managing Director effective immediately.

Continue reading

Women in engineering profile: Lesley D. Frame

June 9, 2016
Source: ASM International

Women in engineering profile: Lesley D. Frame

This new profile series introduces leading materials scientists from around the world who happen to be females. Here we speak with Lesley D. Frame, Director of Product Development for Thermatool Corp.

Continue reading

IMS Welcomes the Failure Analysis Society

June 2, 2016
Source:

Hello IMS Members,

On behalf of the International Metallographic Society and its board of directors, I would like to welcome the new ASM affiliate, the Failure Analysis Society. The society is dedicated to advancing the important role failure analysis plays in the materials science industry. The new affiliate society emerged from an existing ASM committee that has offered failure analysis programming and content for more than 15 years. Currently, FAS has approximately 2500 members.

FAS will continue to provide collaboration, networking, and educational opportunities for materials science professionals. It will also continue to have its own technical programming at the annual Materials Science & Technology conference, and will continue to publish its own journal, the Journal of Failure Analysis and Prevention. In addition, an online database of failure analysis case studies will be available in the future.

Metallographic evaluation, interpretation, and expertise are an integral tool to the world of failure analysis. There is a common bond between our two affiliate societies. Our members should welcome to the opportunity to collaborate with this new ASM affiliate society.

FAS is the sixth affiliate society launched by ASM, joining the Heat Treating Society, Thermal Spray Society, International Metallographic Society, Electronic Device Failure Analysis Society, and the International Organization on Shape Memory and Superelastic Technologies.

The FAS membership fee is $25 annually and also requires a membership to ASM International.

Sincerely,

Daniel P. Dennies, Ph.D., P.E., FASM
Director, International Metallographic Society
Director, Failure Analysis Society

 

IMS Welcomes the Failure Analysis Society

On behalf of the International Metallographic Society and its board of directors, I would like to welcome the new ASM affiliate, the Failure Analysis Society.

Continue reading

ASM forms strategic alliance with SVC

May 4, 2016
Source: ASM International

ASM forms strategic alliance with SVC

The new strategic alliance brings the complementary strengths of both organizations together to better serve their global members and the community at large.

Continue reading

Space telescope boasts a dozen flight mirrors

May 3, 2016
Source:

One dozen flight mirrors are now installed on NASA's James Webb Space Telescope, out of the eighteen mirror segments that make up the primary mirror. The assembly of the primary mirror is an important milestone for the Webb telescope, but is just one component of this huge and complex observatory.

Since December 2015, scientists and engineers have been working tirelessly to install all the primary mirror segments onto the telescope structure in the large clean room at NASA's Goddard Space Flight Center, Greenbelt, Md. The twelfth mirror was installed on January 2, 2016.

"This milestone signifies that all of the hexagonal shaped mirrors on the fixed central section of the telescope structure are installed and only the three mirrors on each wing are left for installation," says Lee Feinberg at NASA Goddard. "The incredibly skilled and dedicated team assembling the telescope continues to find ways to do things faster and more efficiently."

Each hexagonal-shaped segment measures just over 4.2 ft (1.3 m) across and weighs approximately 88 lb (40 kg). After being pieced together, the 18 primary mirror segments will work together as one large 21.3-ft (6.5-m) mirror. The primary mirror will unfold and adjust to shape after launch. The mirrors are made of ultra-lightweight beryllium. The mirrors are placed on the telescope's backplane using a robotic arm, guided by engineers. The full installation is expected to be completed soon.

The mirrors were built by Ball Aerospace & Technologies Corp., Boulder, Colorado. Ball is the principal subcontractor to Northrop Grumman, Falls Church, Va., for the optical technology and lightweight mirror system. The installation of the mirrors onto the telescope structure is performed by Harris Corp., Rochester, N.Y. Harris Corp. leads integration and testing for the telescope.

While the mirror assembly is a very significant milestone, there are many more steps involved in assembling the Webb telescope. The primary mirror and the tennis-court-sized sunshield are the largest and most visible components of the Webb telescope. However, there are four smaller components that are less visible, yet critical. The instruments that will fly aboard Webb—cameras and spectrographs with detectors able to record extremely faint signals—are part of the Integrated Science Instrument Module (ISIM), which is currently undergoing its final cryogenic vacuum test and will be integrated with the mirror later this year.

The near infrared spectrograph (NIRSpec) has programmable microshutters which enable observation up to 100 objects simultaneously. The near infrared camera (NIRCam) is equipped with coronagraphs, instruments that allow astronomers to take pictures of very faint objects around a central bright object, like stellar systems.

The Webb telescope also has a cryocooler for cooling the mid-infrared instrument (MIRI) to a very cold 7 K so they can work. MIRI has both a camera and a spectrograph that sees light in the mid-infrared region of the electromagnetic spectrum, with wavelengths that are longer than our eyes see. There's also the Fine Guidance Sensor (FGS) allows Webb to point precisely, so that it can obtain high-quality images.

Over the next two years in preparation for launch, various components of the Webb telescope will endure rigorous environmental and optical testing. The sunshield will be joined with the spacecraft bus (main structure) followed by more testing. The Webb telescope is planned for launch in 2018.

The James Webb Space Telescope is the scientific successor to NASA's Hubble Space Telescope. It will be the most powerful space telescope ever built. Webb is an international project led by NASA with its partners, the European Space Agency, and the Canadian Space Agency.

Image caption — One dozen (out of 18) flight mirror segments that make up the primary mirror on NASA's James Webb Space Telescope have been installed at NASA's Goddard Space Flight Center. Courtesy of NASA/Chris Gunn.

Space telescope boasts a dozen flight mirrors

One dozen flight mirrors are now installed on NASA’s James Webb Space Telescope, out of the eighteen mirror segments that make up the primary mirror.

Continue reading

Heat-treated powder metallurgy titanium alloy has higher strength, lower cost

April 13, 2016
Source:

Pacific Northwest National Laboratory, Richland, Wash., announces that its research team has improved the strength of a titanium alloy by producing it via powder metallurgy and heat treating it at different temperatures, then quenching in cold water.

Five decades ago, metallurgists created an alloy named Ti185 by blending titanium with low-cost iron, aluminum, and vanadium. However, superior strength was observed for this alloy only in some places, and the alloy had a tendency to clump. Iron clustered in some areas, leading to beta fleck defects, making the alloy unsuitable for reliable commercial production.

Subsequently, in a study carried out about six years ago, the PNNL researchers and its collaborators devised a low-cost powder metallurgy process for the industrial-scale production of the alloy. They used titanium hydride powder instead of molten titanium as the starting material, reducing the energy requirements significantly and cutting the process time in half. ADMA co-developed the method with PNNL metallurgist Curt Lavender. The company sells advanced materials such as the titanium hydride powder to industries, including aerospace.

In their earlier study, the researchers had already demonstrated the superior mechanical properties of the titanium alloy created from their low-cost process. In the new study, they explored how to make even stronger titanium alloys. The team  was able to gain insights into the nanostructure of the alloy by using a unique atom probe imaging approach and powerful electron microscopes.

Using electron microscopy, the team observed the microstructure of the alloy at a resolution of hundreds of nanometers. The atom probe tomography system at the Environmental Molecular Sciences Laboratory, a DOE Office of Science User Facility located at PNNL, was used to observe the arrangement of individual atoms in 3D.

The researchers found that their optimized heat-treating process produced an alloy with an alpha phase, consisting of micron and nanometer -size precipitate regions, in a matrix of beta phase. Each region has higher concentrations of certain elements. The aluminum and titanium atoms are found inside the nano-sized alpha phase precipitates, whereas vanadium and iron are in the beta phase.

"We found that if you heat treat it first at a higher temperature before a low -temperature heat  treatment step, you could create a titanium alloy 10 to 15% stronger than any commercial titanium alloy currently on the market, and that it has roughly double the strength of steel," says Arun Devaraj, Materials Scientist at PNNL

"This alloy is still more expensive than steel, but with its strength-to-cost ratio, it becomes much more affordable with greater potential for lightweight automotive applications," added Vineet Joshi, who serves as a metallurgist at PNNL.

www.pnnl.gov

Heat-treated powder metallurgy titanium alloy has higher strength, lower cost

Pacific Northwest National Laboratory, Richland, Wash., announces that its research team has improved the strength of a titanium alloy by producing it via powder metallurgy and heat treating it at different temperatures, then quenching in cold water.

Continue reading

3D-printed metal aircraft parts

April 8, 2016
Source:

Alcoa, Pittsburgh, entered into an agreement with Airbus, France, to supply 3D-printed metal parts for commercial aircraft. The parts will be produced using comprehensive capabilities—from multimaterial alloy development to additive manufacturing and aerospace parts qualification. The first additive manufactured parts are expected to be delivered midyear.

The agreement draws on Alcoa's aerospace experience and new technologies gained through its recent acquisition of RTI. The company also recently invested in 3D-printing and metallic powder production capabilities at its technical center outside of Pittsburgh.

Last year, Alcoa acquired RTI International Metals (RTI)—now known as Alcoa Titanium & Engineered Products (ATEP)—which grew its additive manufacturing capabilities to include 3D-printed titanium and specialty metals parts produced at ATEP's Austin, Texas facility. The Airbus agreement draws on these capabilities as well as ATEP's titanium ingot melting and billetizing, machining, finishing, and inspection technologies.

Alcoa will use advanced CT scan and hot isostatic pressing (HIP) capabilities at its advanced aerospace facility in Whitehall, Mich. HIP strengthens the metallic structures of traditional and additive manufactured parts made of titanium and nickel based superalloys. Through a $22 million investment in the technology, Alcoa today owns and operates one of the largest aerospace HIP technology complexes in the world.

Additionally, Alcoa is bolstering its additive manufacturing capabilities through a $60 million expansion in advanced 3D-printing materials and processes, including metallic powders. The expansion is located at the Alcoa Technical Center near Pittsburgh.

3D-printed metal aircraft parts

Alcoa, Pittsburgh, entered into an agreement with Airbus, France, to supply 3D-printed metal parts for commercial aircraft.

Continue reading