Two new car bottom furnace contracts awarded to Can-Eng

August 7, 2021
Source: ASM International

Two new car bottom furnace contracts awarded to Can-Eng

Can-Eng Furnaces International, Niagara, N.Y., has been awarded a contract to design and manufacture two 50,000 lb/hr. car bottom furnaces for one of the largest metals and mining companies in the world.

Continue reading

Solar Atmospheres vacuum heat treats longest nickel alloy tubes ever


Source: ASM International

Solar Atmospheres vacuum heat treats longest nickel alloy tubes ever

Solar Atmospheres of Western Pennsylvania, Hermitage, Pa., successfully vacuum heat treated the largest and longest load of nickel alloy tubing ever in a commercial vacuum furnace. They were able to preserve the brightness and cleanliness of a 45-foot-long seamless tubing while meeting extremely stringent mechanical properties.

Continue reading

One Minute Mentor: Effect of porosity on the heat treatment of powder metallurgy steels

July 24, 2021
Source: ASM International

One Minute Mentor: Effect of porosity on the heat treatment of powder metallurgy steels

Porosity has the greatest single effect on the response of PM Steels to heat treatment compared with conventional steels. The majority of parts have a porosity between 5 and 15 vol%, far more than is found in a typical casting. Every mechanism in press and sinter is subject to diminishing returns; i.e., compact density has a decreasing dependence on compaction pressure, as does sintering and homogenization.

Continue reading

Constellium to sponsor skilled trades scholarships

June 26, 2021
Source: ASM International

Constellium to sponsor skilled trades scholarships

Constellium, Paris will sponsor ten new skilled trades scholarships at West Virginia University, Parkersburg. Now in its second year, the program provides financial assistance to selected high school graduates to help them earn an associate degree in Multi-Craft Technology or Reliability and Maintenance Technology.

Continue reading

One Minute Mentor: Sintering of power particles

May 29, 2021
Source: ASM International

One Minute Mentor: Sintering of power particles

During sintering, metallurgical bonds form between powder particles. Strength, ductility, toughness, and electrical and thermal conductivities increase with increasing density. If different materials were blended together, interdiffusion could promote the formation of alloys and intermetallic phases. As a consequence of the density increases, size decreases.

Continue reading

Seco/Warwick introduces Zeroflow


Source: ASM International

Seco/Warwick introduces Zeroflow

Seco/Warwick, Poland, has introduced a new gas nitriding technology called ZeroFlow to the global industry in cooperation with scientists from the Poznan University of Technology. ZeroFlow reduces process costs while providing more ecologically friendly performance.

Continue reading

NanoAL brings Addalloy to Mitsubishi


Source: ASM International

NanoAL brings Addalloy to Mitsubishi

NanoAL LLC, Boston, has signed a commercial license agreement with Mitsubishi Corp. RtM Japan Ltd. to bring its Addalloy family of advanced aluminum alloy powders to the metal additive manufacturing market in Asia.

Continue reading