C.I. Hayes installs conveyor belt atmosphere furnace

January 25, 2016
Source:

C.I. Hayes, a Gasbarre Furnace Group Company, Cranston, R.I., reports the installation of a Model BAC-M Conveyor Belt Atmosphere Furnace designed for various processes such as brazing, hardening, and annealing of stainless steel materials. The multi-zoned electric furnace is equipped with a conveyor belt drive and silicon carbide heating elements, as well as a controlled hydrogen atmosphere.

The furnace includes an analyzer used to monitor dewpoint and oxygen levels for process and safety purposes. The brick-lined heating chamber, which includes a silicon carbide hearth that supports an Inconel muffle, is designed to operate to 2100°F. The 18-inch wide conveyor belt provides a six-inch work clearance and travels through a 60-inch effective heated length.

C.I. Hayes designs, manufactures and services industrial vacuum and atmosphere heat treating equipment and has been delivering custom solutions to the heat treating industry for 109 years.

www.cihayes.com

www.gasbarrefurnacegroup.com

 

 

C.I. Hayes installs conveyor belt atmosphere furnace

C.I. Hayes, a Gasbarre Furnace Group Company, Cranston, R.I., reports the installation of a Model BAC-M Conveyor Belt Atmosphere Furnace designed for various processes such as brazing, hardening, and annealing of stainless steel materials.

Continue reading

Ipsen vacuum furnaces deployed for aerospace, automotive, and additive manufacturing


Source:

Ipsen, Cherry Valley, Ill., announces that over the past month, the company has shipped four furnaces and one upgrade for a variety of applications and industries. These shipments included three Titan vacuum furnaces that shipped within a span of two weeks; a horizontal MetalMaster vacuum furnace; and a custom furnace upgrade:

The Titan H6 with 2-bar absolute pressure was shipped to a U.S. manufacturer, where it will be used to process parts for the additive manufacturing industry.

Another Titan H6 with 2-bar absolute pressure was shipped to a company in  the aerospace industry – a market where Ipsen and its equipment have a strong reputation and presence.

The Titan H4 with 2-bar absolute pressure was shipped to California, and will also be used to process parts for the Aerospace industry.

The horizontal MetalMaster with a 48 x 72 x 48-inch graphite work zone was shipped to Alabama, where it will be used to process automotive parts..

The custom furnace upgrade was shipped to Georgia for a company in the aerospace industry, and it will allow the the company to enhance its furnace performance and ensure continued high-quality results.

With custom-tailored hot zones, controls, and mechanical upgrades and retrofits for both vacuum and atmosphere furnaces, Ipsen is able to deliver solutions that expand capabilities, increase flexibility and extend the life of equipment. Ipsen's engineers can also help adjust, modify, and upgrade equipment and controls to achieve peak performance and minimize downtime.

www.IpsenUSA.com

 

Ipsen vacuum furnaces deployed for aerospace, automotive, and additive manufacturing

Ipsen, Cherry Valley, Ill., announces that over the past month, the company has shipped four furnaces and one upgrade for a variety of applications and industries.

Continue reading

Tribogenics XRF analyzer is based on a cartridge system instead of glass X-ray tube


Source:

Tribogenics, Los Angeles, Calif., introduces the Watson XRF analyzer, in which the company says conventional glass X-ray tubes are replaced with an X-Change cartridge system that makes changing cartridges "as easy as changing the ink in an inkjet printer." It enables quick and accurate identification of 32 elements, and can reportedly identify most of the popular aluminum alloys in less than twenty seconds.

Watson software is said to be able to identify more than 436 metal alloys and provide identification and analysis of more than 32 of the most common elements used in tens of thousands of alloy grades.

Watson uses the Android operating system and supports the mobile user interface concepts and wireless communication interfaces. This permits a wide range of personnel, with varying levels of skill and knowledge, to quickly and accurately use the Watson for all types of applications that can use hand-held XRF technology. The software supports configuring the XRF instrument and performs automatic internal calibration without the need for a trained technician or carrying around bulky calibration discs.

It takes advantage of the latest in smartphone design and software, and costs $10,000. An intuitive interface means that it's easy for anyone to use without any special training. Watson is Wi-Fi enabled for automatic software updates, and comes with integrated market pricing, keeping users current on all local alloy market prices.

www.tribogenics.com

 

Tribogenics XRF analyzer is based on a cartridge system instead of glass X-ray tube

Tribogenics, Los Angeles, Calif., introduces the Watson XRF analyzer, in which the company says conventional glass X-ray tubes are replaced with an X-Change cartridge system that makes changing cartridges “as easy as changing the ink in an inkjet printer.”

Continue reading

One Minute Mentor: Secondary Hardening in Tool Steels

January 22, 2016
Source:

As shown schematically in the graph, high-temperature hardness is made possible only by a very important straightening mechanism: secondary hardening, promoted by the precipitation of fine alloy carbides. The stronger the secondary hardening (meaning more intense carbide precipitation), the higher the tempering resistance of hot-work tool steels. Such precipitation intensity depends on the amount of alloy elements in solid solution, which is related to the alloy composition and heat treating practice obtained by molybdenum, vanadium, or tungsten alloying. 

The graph shows a schematic of hardness after tempering and the effect of secondary hardening in high-alloy steels. Observe that high-temperature hardness is only possible through precipitation hardening caused by alloy carbides (secondary hardening). At low temperatures, hardness is less than martensite due to the presence of retained austenite, which is eliminated after high-temperature tempering.

Volume 4D, Heat Treating of Irons and Steels â‡’ Tool Steels ⇒ Heat Treating of Hot-Work Tool Steels ⇒ Introduction 

One Minute Mentor: Secondary Hardening in Tool Steels

As shown schematically in the graph, high-temperature hardness is made possible only by a very important straightening mechanism: secondary hardening, promoted by the precipitation of fine alloy carbides.

Continue reading

Bruker introduces MultiMode 8-HR atomic force microscope for nanoscale research

January 20, 2016
Source:

Bruker Nano Surfaces, Santa Barbara, Calif., announces that it has significantly enhanced the capabilities of its MultiMode platform with the MultiMode 8-HR. Improvements include higher speeds, higher resolution imaging, new capabilities in nanomechanics with enhanced PeakForce QNM, and new FastForce Volume modes. These improvements are also available as upgrades to current MultiMode systems.

The high-resolution and data processing capabilities of the MultiMode 8-HR are the result of its combination of rigid mechanical design and extremely advanced control electronics. Utilizing Bruker's NanoScope  V Controller and new Version 8.2 software, the system features unprecedented bandwidth and extremely low-noise data acquisition to enable such proprietary technology advances as ScanAsyst, Peak Force QNM and FastForce Volume. These features combine to reaffirm the MultiMode 8-HR as the most versatile, highest performance AFM in its class.

www.bruker.com

 

Bruker introduces MultiMode 8-HR atomic force microscope for nanoscale research

Bruker Nano Surfaces, Santa Barbara, Calif., announces that it has significantly enhanced the capabilities of its MultiMode platform with the MultiMode 8-HR.

Continue reading

Bodycote produces interactive History of Metallurgy from across time and continents

January 19, 2016
Source:

Bodycote, England, has produced an Interactive History of Metallurgy, a look back at the long history of metal processing and heat treatment. Containing over 200 high quality images and numerous videos, Bodycote pays homage to the artisans from thousands of years ago along with the scientists and inventors of more modern metallurgy and engineering.

Starting in 8700BC with the world's oldest known copper artifacts, all the way through to the modern processes that Bodycote undertakes daily, the resource charts the development of metal working from the mystical and utilitarian requirements of early mankind, through to the scientific and technical breakthroughs of the 20th century.

Bodycote, the leader in an industry that dates back thousands of years, developed the interactive resource to explore the evolution of metallurgy and heat treating and to acknowledge the collective work of scientists and engineers. Their hard work and discoveries have enhanced the properties of metals and alloys, making them deliver safer, more durable results for more and more applications.

Visit the Interactive History of Metallurgy at http://www.bodycote.com/history-of-metal.

 

Bodycote produces interactive History of Metallurgy from across time and continents

Bodycote, England, has produced an Interactive History of Metallurgy, a look back at the long history of metal processing and heat treatment.

Continue reading

Worthington Industries acquires brazing manufacturer


Source:

Worthington Industries Inc., Columbus, Ohio, has acquired the business of NetBraze LLC, a manufacturer of brazing alloys, silver brazing filler metals, solders, and fluxes primarily used in plumbing, HVAC-R, industrial gas, and OEM markets.

"This acquisition expands our offering of alloys in the professional wholesale channel with innovative products that utilize patented technologies," said Worthington Industries' Pressure Cylinders President Andy Billman." The products that NetBraze has developed save an operator time, resources, and cost when brazing. We look forward to offering these new products in addition to our full complement of joining technologies products to our customers."

Worthington manufactures and distributes a full line of joining alloys including lead-free solders, brazing rods, fluxes, hand torches and hand-torch fuel under the Worthington Joining Technologies and Bernzomatic brands.

NetBraze products include standard BCuP brazing alloys, BAg silver solders and fluxes, and innovative technologies including QuickCoil, which offers up to 22-feet of non-stop brazing, eliminating leftover scrapped stubs produced by traditional brazing rods, and products with lower braze temperatures that make the brazing process more efficient. NetBraze is located in Mt. Orab, Ohio and has 23 employees.

www.worthingtonindustries.com

 

Worthington Industries acquires brazing manufacturer

Worthington Industries Inc., Columbus, Ohio, has acquired the business of NetBraze LLC, a manufacturer of brazing alloys, silver brazing filler metals, solders, and fluxes primarily used in plumbing, HVAC-R, industrial gas, and OEM markets.

Continue reading

Tresa Pollock named Principal Editor for Metallurgical and Materials Transactions


Source: ASM International

Tresa Pollock named Principal Editor for Metallurgical and Materials Transactions

ASM International, Materials Park, Ohio, announces that the new principal editor of the Metallurgical and Materials Transactions (Met Trans) family of journals will be Dr. Tresa M. Pollock, an internationally recognized leader in the science and technology of advanced structural alloys.

Continue reading

Wisconsin Oven gas-fired walk-in batch oven treats industrial transformers

January 18, 2016
Source:

Wisconsin Oven Corp., East Troy, Mich., has shipped a gas-fired walk-in batch oven to an industrial transformer supplier for baking out transformers. The customer opted to add the turn-key installation package, which includes everything from unloading the equipment to commissioning the equipment into operation. The walk-in industrial oven has a maximum temperature rating of 300°F and work chamber of 10 x 10 x 10 feet. The recirculation system was designed with combination airflow to maximize heating rates and temperature uniformity of the products. The heating system utilizes an air heat burner rated at 750,000 BTU per hour.

The turn-key installation service for the industrial oven involved three consecutive days of installation with start-up and training at the facility by two Wisconsin Oven factory technicians.

The turn-key installation included reassembly and rewiring all components removed from shipping; connecting customer's utilities to the equipment; debugging and start-up of equipment;  training three personnel on operation and maintenance; and other installation procedures.

This walk-in batch oven was fully factory tested and adjusted prior to shipment to help reduce installation and start-up times. A 150 point Quality Assurance check list was completed to ensure the equipment met all Wisconsin Oven quality standards.

The industrial batch ovens are backed by Wisconsin Oven's 5-Year WOW warranty, which covers all materials for all components (less wear items).

www.wisoven.com

 

 

Wisconsin Oven gas-fired walk-in batch oven treats industrial transformers

Wisconsin Oven Corp., East Troy, Mich., has shipped a gas-fired walk-in batch oven to an industrial transformer supplier for baking out transformers.

Continue reading

J.L. Becker Co. delivers temper furnace to auto parts supplier in Mexico


Source:

J.L. Becker, a Gasbarre Furnace Group Company, Plymouth, Mich., has delivered a 36 x 72 x 36-inch gas-fired box temper furnace to a major Tier 1 automotive components supplier in Mexico. The furnace is designed to hold a 6000-pound gross load, with a maximum operating temperature of 1350°F.

Process capabilities include tempering and stress relief. This furnace comes complete with a stationary load table equipped with a newly designed motor-driven roller chain and handler head assembly. The new drive system provides superior performance, more accurate positioning, and ease of setup and maintenance.

The equipment includes both batch and continuous systems. The company specializes in Integral Quench, Tip Up, Box, and Car Bottom furnaces, as well as a full line of replacement parts and auxiliary equipment, including atmosphere generators, quench tanks, and charge cars.

www.jlbecker.com and www.gasbarrefurnacegroup.com

 

 

J.L. Becker Co. delivers temper furnace to auto parts supplier in Mexico

J.L. Becker, a Gasbarre Furnace Group Company, Plymouth, Mich., has delivered a 36 x 72 x 36-inch gas-fired box temper furnace to a major Tier 1 automotive components supplier in Mexico.

Continue reading