One Minute Mentor: Heat Treating of Hot-Work Tool Steels

January 15, 2016
Source:

The ability of a given grade of hot-work tool steel to maintain hardness for a prolonged time at high temperatures is called tempering resistance. A simple comparison of tempering resistance may be performed by analyzing tempering curves such as those shown in the graph. Higher tempering resistance is related to curves dislocated to the right. High mechanical strength at high temperature is fundamental for hot-work steels.

Toughness in hot-work tools is an essential property for avoiding the cracks and fractures that can be common in normal working conditions. Unexpected and very unstable in cold-work tools, cracks may be encountered after a given operation time for hot-work dies. The most important example is fine crack networks, large in number but small in length, observed on a tool surface after the tooling operation. This kind of cracking is known as heat checking and is typically found in die-casting dies as well as in forging dies or other hot-work tools. The cause is thermal fatigue at the tool surface, caused in turn by repeated temperature fluctuations (heating and cooling) during tool operation.

Depending on the intensity, heat checking can lead to tool failure, which is typically the case in die-casting cavities. In such situations, the casting metal, normally aluminum, enters into the heat-checking cracks, making part extractions difficult or impairing part surface quality. In cases of a lack of toughness, gross cracking may also occur, leading to complete loss of the working tool.

Volume 4D, Heat Treating of Irons and Steels -> Tool Steels -> Heat Treating of Hot-Work Tool Steels-> Introduction 

One Minute Mentor: Heat Treating of Hot-Work Tool Steels

The ability of a given grade of hot-work tool steel to maintain hardness for a prolonged time at high temperatures is called tempering resistance.

Continue reading

New international location for ASM heat treating show

January 14, 2016
Source:

ASM International, Materials Park, Ohio, announces that organizers for Heat Treat Mexico are currently seeking abstract submissions on heat treating topics for the upcoming new event in Queretaro, Mexico, to be held later this year in September. It is the first show by the ASM Heat Treating Society specifically focused  on thermal processing technology in Mexico, and organizers expect to reach a broad audience of heat treating professionals. As the January 22nd deadline to submit approaches, organizers encourage the heat treating community to submit their research and take advantage of the opportunity to present at Heat Treat Mexico.

The organization of this technical program is slightly different from other heat treating shows from HTS, as it will focus on three overarching topics, one on each of the three days: Process, Meaning to metallurgy, and Application.

The technical program is organized to emphasize how the materials respond to thermal treatment.  Attendees will gain a higher level of understanding for several methods of heat treating, such as vacuum carburizing,  nitriding, and induction hardening. This unique opportunity highlights the fundamentals of the process on day one.  Changes to the metallurgical structure that result from the treatment will be covered on day two, and control methodology and maintenance protocols important to the specific technology will be highlighted on day three.

Robert J. Madeira, Vice President of Heat Treating for Inductoheat Inc., thinks that attendees will find great value in this show. "ASM International and its legion of industry professional recognize the opportunity to bring its expertise in education to Mexico.  The "Basics of Metallurgy" course and the three day Heat Treating Symposium will be taught simultaneously in Spanish and English. This content-rich forum is designed to deliver expert knowledge about how modern thermal treatments transform metals.  It offers the foundation for understanding that leads to good decisions on the factory floor."

To submit an abstract for Heat Treat Mexico, visit the Heat Treat Mexico website and select your preferred topic, along with the specific facet.  For example, "Induction Heat Treating; What is the Process?" Presenting authors will be notified in February 2016 as to the status of their abstract.

Visit www.asminternational.org/htmexico to submit by January 22, 2016.

####

About ASM International

As the world's largest association of materials-centric engineers and scientists, ASM International is dedicated to informing, educating, and connecting the materials community. A member and volunteer based organization, ASM serves as a central resource that gathers the latest applied information from the field and disseminates it back to industry, academia, and government through published content, classes, conferences, expositions, and local chapter engagement.

To learn more about ASM International, visit www.asminternational.org.

About The ASM Heat Treating Society

HTS, an Affiliate Society of ASM International formed in 1994, is the world's largest network of heat treaters. HTS members work to provide events and services to serve their worldwide membership of captive and commercial heat treaters, equipment manufacturers, researchers, governments and technicians. HTS members have their own unique leadership and agenda to serve the global heat treating community, and are dedicated to: Bringing heat treaters together to discuss heat treating challenges; providing the technical information, knowledge and education needed by all heat treaters; serving as a central clearinghouse for information of value to heat treaters; and interfacing with all organizations that serve heat treaters.

To learn more about HTS, visit www.asminternational.org/hts3-new

New international location for ASM heat treating show

ASM International, Materials Park, Ohio, announces that organizers for Heat Treat Mexico are currently seeking abstract submissions on heat treating topics for the upcoming new event in Queretaro, Mexico, to be held later this year in September.

Continue reading

Liquidmetal amorphous alloy in hybrid knife is 25% harder than stainless steel

January 13, 2016
Source:

Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., has developed the Liquidmetal Hybrid Knife, manufactured of LM105 amorphous alloy by the Liquidmetal process. The 5.25-inch-long hybrid knife embodies a geometry that is not practical to produce with any other metalforming process. A 0.0005-inch fit between the blade and protector is made possible with the ultra-precise Liquidmetal process that can produce parts with features down to eight ten-thousands of an inch.

The barrel hinge implemented utilizing Python programming results in an easy-to-assemble and disassemble two-piece knife with no weak points throughout the open-and-close rotation. The alloy provides as-molded 563 Vickers hardness (25% greater than 17-4PH stainless steel), 1524 MPa yield strength (twice that of titanium), and 1.8% elasticity (four times that of hardened 420 stainless steel). Cultivated by an abundance of scientific data, the hybrid knife and Liquidmetal process stand in a league of their own. Not to be overlooked, the artistic and distinctive design brings a powerful process and set of material properties to life.

Liquidmetal also announces that it has shipped a pre-production order to CoNextions Medical for a key component to be used for suture-based tendon repairs. The initial parts delivery will be used to complete various tests, and will be followed by a full production shipment currently scheduled for early 2016. This delivery represents the ongoing manufacturing solutions for CoNextions design efforts that are taking advantage of the Liquidmetal materials and molding technology.

In addition, Liquidmetal has received its formal ISO 9001:2008 certification, adding an important quality accreditation to the company.

"Our business has a strong commitment to ongoing quality and customer satisfaction. Receiving our ISO certification exemplifies that," said Paul Hauck, Vice President of World-Wide Sales and Marketing. "Our ISO certification will help build customer confidence in our attention to quality."

"The Liquidmetal organization did an admirable job implementing the ISO 9001 standard and passing its certification audit in an impressive 9 months," said Tom Steipp, CEO and President of Liquidmetal Technologies. "Achieving this result was no small undertaking. Every individual in the company played a critical role and it's a testament to the organization's focus on quality."

www.liquidmetal.com

 

Liquidmetal amorphous alloy in hybrid knife is 25% harder than stainless steel

Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., has developed the Liquidmetal Hybrid Knife, manufactured of LM105 amorphous alloy by the Liquidmetal process.

Continue reading

Alcoa to supply GE Aviation with superalloy, titanium, and aluminum components


Source:

Alcoa, Pittsburgh, has signed a long-term contract with GE Aviation for jet engine components made of advanced nickel-based superalloys, titanium, and aluminum for a broad range of GE Aviation engine programs. The agreement is valued at more than $1.5 billion over the contract life.

"We greatly appreciate GE's continued confidence in Alcoa's aerospace capabilities, and are proud to support its advanced jet engine programs through this agreement," said Alcoa Chairman and Chief Executive Officer Klaus Kleinfeld.

Alcoa will employ advanced manufacturing capabilities to produce the parts across several facilities, including LaPorte, Indiana; Whitehall, Michigan; Hampton, Virginia; Dover, New Jersey; Wichita Falls, Texas; Winsted, Connecticut; Dives, France; and Laval, Canada.

Alcoa Power and Propulsion, a major business unit of Alcoa, is the number one supplier of nickel-based superalloy airfoils for jet engine and industrial gas turbine applications. It is also a leading supplier of structural castings made of titanium, aluminum and superalloy for aero engines and airframes. Additional value-add products and services include additive manufacturing, vacuum melted alloys, advanced airfoil coatings and machining, hot isostatic pressing and research & development. With 20 global production facilities, Alcoa Power and Propulsion employs more than 9600 people worldwide.

www.alcoa.com

 

Alcoa to supply GE Aviation with superalloy, titanium, and aluminum components

Alcoa, Pittsburgh, has signed a long-term contract with GE Aviation for jet engine components made of advanced nickel-based superalloys, titanium, and aluminum for a broad range of GE Aviation engine programs.

Continue reading

Ipsen offers heat treating courses in February, April, June, August, and October

January 12, 2016
Source:

Ipsen, Cherry Valley, Ill., announces that it plans to host another series of Ipsen U classes throughout 2016, with courses available February 2-4, April 5-7, August 2-4 and October 11-13.

A class will also be offered in June, with more details coming soon. These three-day courses provide attendees with a broad overview of furnace equipment, processes and maintenance, as well as a hands-on approach to learning while receiving qualified tips directly from the experts. They view the different furnace components firsthand while learning how they affect other parts of the furnace and/or specific processes.

Reflecting on past courses, attendees commented that "staff and facility are top notch and very knowledgeable in the heat-treating process." Another participant praised the instructors' "incredible amount of knowledge, hints, tips and real world advice." Others found it useful to "see all of the different furnace designs and be able to relate them to the information talked about earlier in the class," concluding that "mixing the lecture with actual furnace visualization was extremely valuable."

Throughout the course, attendees are able to learn about an extensive range of topics – from an introduction to vacuum and atmosphere furnaces, to heat treating, furnace controls, subsystems, maintenance, and more. 

Overall, Ipsen U allows participants to build and refresh their knowledge of heat-treating equipment and processes through applied learning. Regardless of where you fall on the expertise scale – maintenance, operator, engineer, project manager, and/or plant manager – Ipsen U's instructors will provide the necessary level of information in a casual, open-forum environment.

www.ipsenusa.com/ipsenu

 

Ipsen offers heat treating courses in February, April, June, August, and October

Ipsen, Cherry Valley, Ill., announces that it plans to host another series of Ipsen U classes throughout 2016, with courses available February 2-4, April 5-7, August 2-4 and October 11-13.

Continue reading

2016 Bernard M. Gordon Prize awarded to Worcester Polytechnic Institute


Source:

The 2016 Bernard M. Gordon Prize for Innovation in Engineering and Technology Education is awarded to Worcester Polytechnic Institute educators Diran Apelian, FASM, (pictured), Arthur C. Heinricher, Richard F. Vaz, and Kristin K. Wobbe, "for a project-based engineering curriculum developing leadership, innovative problem-solving, interdisciplinary collaboration, and global competencies."

The project-based engineering curriculum at WPI prepares 21st century leaders to tackle global issues through interdisciplinary collaboration, communication, and critical thinking. The Institute's engineering program engages students with a specially designed sequence in which first-year students complete projects on topics such as energy and water; second-year capstones focus on the humanities and arts; junior-year interdisciplinary projects relate technology to society; and senior design projects are done in conjunction with external sponsors, providing relevant experience upon graduation.

Last year, WPI launched its Institute on Project-Based Learning, an initiative to help other colleges and universities make progress toward implementing project-based learning on their campuses.

The Bernard M. Gordon Prize for Innovation in Engineering and Technology Education is one of the most prestigious awards in engineering education

https://www.nae.edu/default.aspx?id=148200

 

2016 Bernard M. Gordon Prize awarded to Worcester Polytechnic Institute

The 2016 Bernard M. Gordon Prize for Innovation in Engineering and Technology Education is awarded to Worcester Polytechnic Institute educators Diran Apelian, FASM, (pictured), Arthur C. Heinricher, Richard F. Vaz, and Kristin K. Wobbe, “for a project-based engineering curriculum developing leadership, innovative problem-solving, interdisciplinary collaboration, and global competencies.”

Continue reading

Solar Atmospheres’ Greenville facility offers a range of vacuum processing capabilities


Source: ASM International

Solar Atmospheres’ Greenville facility offers a range of vacuum processing capabilities

Solar Atmospheres, Greenville, S.C., reports that its newest facility now has a wide range of vacuum processing capacity available, from furnaces suited for small lots and development cycles, to a 24-foot long vacuum chamber capable of processing up to 50,000 pounds at 2650°F.

Continue reading

Bodycote opens new plants in Georgia and South Carolina


Source:

Bodycote, U.K., announces two new heat treatment plants in the southeastern United States: Covington, Ga., and Greenville, S.C.  The Covington plant will open in Spring 2016 to replace the nearby Conyers facility. Primarily serving automotive and general industrial customers, the new plant will be more than double the size of the existing Conyers facility, immediately increasing capacity to serve the Georgia and Florida marketplaces. 

The Greenville plant is a new Nadcap-accredited facility that will serve the region's aerospace manufacturing supply chains. It is scheduled to be operational mid-2016 and provides further expansion opportunities to install additional key services in response to customer demand.

These new facilities are part of Bodycote's investment and expanded services strategy to serve the diverse range of industries in the Southeast United States.

Through heat treatment, metal joining, surface technology, and hot isostatic pressing, Bodycote improves the properties of metals and alloys, extending the life of vital components for a wide range of industries, including aerospace, defense, automotive, power generation, oil & gas, construction, medical and transportation.

www.bodycote.com

 

Bodycote opens new plants in Georgia and South Carolina

Bodycote, U.K., announces two new heat treatment plants in the southeastern United States: Covington, Ga., and Greenville, S.C.

Continue reading

One Minute Mentor: Relation Between Tempering Temperature and Hardness

January 8, 2016
Source:

The graphs show the relation between tempering temperature and hardness for D2 and D3 tool steels. Steels were austenitized in an air furnace; a recirculating pit-type furnace was used for tempering. The curves represent steel from three suppliers. An average of five hardness measurements were made on each specimen from each supplier. Specimens were 25 mm (1 in.) in diameter and 38 mm (1.5 in.) long.

It can be seen that certain steels exhibit higher hardness after being tempered at about 540°C (1000 °F) than after being tempered at temperatures 55 to 110°C (100 to 200°F) lower. This reversal in the usual relationship is known as secondary hardening and is caused by transformation of retained austenite and the precipitation of fine alloying carbides during tempering at the higher temperatures, near 540 °C (1000 °F).

Volume 4D, Heat Treating of Irons and Steels -> Tool Steels -> Heat Treating of Cold-Work Tool Steels -> Medium-Alloy Air-Hardening, High-Carbon High-Chromium and High-Vanadium-Powder Metallurgy Steels -> Recommended Heat Treating Practices  

One Minute Mentor: Relation Between Tempering Temperature and Hardness

The graphs show the relation between tempering temperature and hardness for D2 and D3 tool steels.

Continue reading

Seco-Warwick retrofits mesh belt furnace to increase productivity by 40%


Source:

Seco-Warwick, Meadville, Pa., announces that a major U.S.-based manufacturer is improving efficiency by retrofitting its mesh belt furnace originally commissioned by Seco-Warwick nearly 20 years ago. The goal of the project is to increase productivity 40% by fully automating the material handling system that moves small forgings from the forge press into the furnace with minimal operator intervention.

In addition to an improved loading rate, the mesh belt will be updated to reduce scrap rates. During an initial evaluation, it was also determined that the cooling efficiency could be improved by replacing the original water-cooled carbon steel chamber with a newly designed stainless steel chamber that will resist corrosion, speed cooling, and extend the useful life of the equipment.

Seco-Warwick will provide the engineering, fabrication and commissioning of a stainless steel cooling chamber, improved mesh belt design and a fully automated loading system from their Meadville, PA facility. The system is scheduled for operation by May 2016.

www.secowarwick.com

 

Seco-Warwick retrofits mesh belt furnace to increase productivity by 40%

Seco-Warwick, Meadville, Pa., announces that a major U.S.-based manufacturer is improving efficiency by retrofitting its mesh belt furnace originally commissioned by Seco-Warwick nearly 20 years ago.

Continue reading