New CFRC Info and Performance in Oil Quenching

July 17, 2018
Source: ASM International

New CFRC Info and Performance in Oil Quenching

For decades, successful manufacturers of precision parts used heat treating fixtures made of various alloy materials, but over time, these alloys would become distorted and embrittled.

Continue reading