One Minute Mentor: Corrosion Resistance of Carburized 316 Steel
January 8, 2018
Source: ASM International
Electrochemical polarization curves show a 600 to 800 mV increase in pitting potential in treated (900 to 1000 mV) versus nontreated (200 to 300 mV) type 316 in chloride solutions.
Continue reading
Baker Furnace ships record number of custom and standard furnaces in 2017
January 4, 2018
Source: ASM International
Baker Furnace, Brea, Calif., announces record shipments of custom and standard units in a variety of configurations, thanks to its new facility with 40,000 square feet of manufacturing space.
Continue reading
Despatch redesign cuts 20 inches from the width of its RAD2-19 cabinet ovens
Source: ASM International
Despatch, Minneapolis, Minn., has redesigned its RAD2-19 and RFD2-19 cabinet ovens to accommodate its customers’ need for a smaller footprint.
Continue reading
New press brake and swing beam shear led to higher furnace sales for Lindberg MPH in 2017
Source: ASM International
Lindberg MPH, Riverside, Mich., reports that, in the beginning of 2017, the company purchased an Ermak press brake and hydraulic swing beam shear to maximize production capabilities.
Continue reading
Indirect gas-fired aluminum aging oven treats exterior components of aircraft engines
Source: ASM International
Wisconsin Oven Corp., East Troy, Wis., has built an indirect gas-fired aluminum aging oven for treating aluminum exterior components of aircraft engines.
Continue reading
Aleris secures multi-year contract with Embraer for aluminum flat-rolled products
January 3, 2018
Source: ASM International
Aleris, Cleveland, has signed a new multi-year contract with Embraer to supply aluminum flat-rolled products for use in the production of all Embraer aircraft.
Continue reading
Constellium receives defense award for large scale aluminum hull that protects warfighters
Source: ASM International
Constellium N.V., Netherlands, has received the 2017 Defense Manufacturing Technology (ManTech) Achievement Award in the category of Enhancing Military Capability, for its contributions as part of the U.S. Army’s Affordable Protection from Objective Threats ManTech program.
Continue reading
Alliance Magnesium extracts magnesium from asbestos tailings by electrolysis process
Source: ASM International
Alliance Magnesium, Brossard, Quebec, has developed a hydrometallurgical process combined with an electrolytic process to extract magnesium from asbestos tailings, which contain 25% magnesium.
Continue reading
Semiautomatic compact abrasive cutoff machine features large operator interface
December 29, 2017
Source: ASM International
ATM GmbH, Germany, introduces the Brillant 240, a compact and flexible semi-automatic abrasive cut-off machine with a ten-inch cut-off wheel for workpieces or samples up to 3.75 inches.
Continue reading
One Minute Mentor: Low-Temperature Carburization of Stainless Steels
December 11, 2017
Source: ASM International
The combination of hardness and ductility achieved by low-temperature carburization also enhances resistance to erosion. The graph shows the results of cavitation testing of treated and nontreated 316 stainless steel specimens.
Continue reading