SAE International MedAccred Heat-Treating Standard recognized by U.S. FDA

January 31, 2018
Source: ASM International

SAE International MedAccred Heat-Treating Standard recognized by U.S. FDA

SAE International, Warrendale, Pa., announces that technical standard AMS2750 – Pyrometry, has received complete recognition by the U.S. Federal Drug Administration Center for Devices and Radiological Health, and it has been added to its list of recognized consensus standards database, List #47.

Continue reading

Heat Treatment with a Turbulent Twist

January 30, 2018
Source: ASM International

Heat Treatment with a Turbulent Twist

Furnace atmosphere circulation is at the heart of the heat treatment process: without thorough circulation of gases, heat treatment processes cannot achieve consistent results in terms of surface quality and mechanical properties.

Continue reading

One Minute Mentor: Crevice Corrosion Testing

January 22, 2018
Source: ASM International

One Minute Mentor: Crevice Corrosion Testing

In crevice corrosion testing, treated 316 stainless steel compares favorably with alloy 625, as shown in the figure with three images. This figure shows three specimens at the end of a weeklong crevice corrosion test in natural seawater, at room temperature, under an applied potential of 300 mV.