Researchers at Harvard’s John A. Paulson School of Engineering and Applied Sciences and the Faculty of Arts and Sciences have developed a new method for making some of the smallest and smoothest curved optical mirrors used to control individual photons. The team, led by professors Marko Lončar, Mikhail Lukin and Kiyoul Yang, created high-performance mirrors that can trap light between them to form state-of-the-art optical resonators operating at near-infrared wavelengths—crucial for manipulating single atoms in quantum computing. The advance could benefit future quantum computers, quantum networks, integrated lasers and environmental sensing technologies.
Optical resonators, also known as optical cavities, are fundamental building blocks of countless light-based devices today, from precision instruments for timekeeping and spectroscopy, to lasers and optical interconnects in data centers. They are like guitar strings, but for light: Only certain wavelengths of light (as opposed to sounds) can fit inside the space between two mirrors and intensify. Increasingly, quantum applications require these same types of optical cavities, but much smaller and with lower signal loss.
The Harvard team’s new microfabrication method, led by first author and former graduate student Sophie Ding, was inspired by a practical problem facing colleagues in experimental physics who are trying to build quantum networks out of ultracold single atoms. They were in search of optical cavities with extremely smooth mirrors that would strongly couple atoms to photons, work at specific wavelengths, and could be scaled and shaped.
“We needed these high-quality photonic interfaces to create efficient ways to have single photons interact with single atoms, allowing for fast, high-fidelity quantum networking,” said paper co-author Brandon Grinkemeyer, a postdoctoral researcher in the Lukin lab.
But most lithography or etching methods today cannot produce sufficiently smooth mirror surfaces for the most demanding quantum applications.
Ding’s new method is an example of working smarter, not harder.
The researchers started with a silicon wafer and used thermal oxidation to grow a thin layer of silicon oxide on the surface, which works to flatten bumps and grooves. When removed, the oxide leaves behind a smooth silicon surface. On that surface, the researchers deposited a precisely engineered stack of transparent oxide layers, called a dielectric mirror coating. When a hole is etched through the back and the coating is freed from the silicon wafer, it buckles into a perfectly curved shape because of built-in mechanical stress, that naturally forms a high-quality mirror.
This process allows the researchers to control the radius of the mirror’s curvature and the wavelengths of light the mirror will reflect, making the method highly scalable and relatively simple.
“In microfabrication, we are sometimes confined by the thought that surface roughness is defined by the etch or the mask, and we try very hard to optimize them,” Ding said. “But when we are using the properties of the materials, we can do a lot less of that and have more robust results.”
The researchers showed their microfabricated resonators could reach a record “finesse” of 0.9 million at a wavelength of 780 nanometers, meaning light can bounce back and forth inside the cavity nearly a million times before scattering. By contrast, optical telecommunications signals transmit at 1550 nanometer wavelengths.
The optical cavities created with Ding’s new method could be used in modular quantum computing applications, in which many atoms are linked together by photons in optical fibers. The cavities would be the critical interfaces that let an atom’s quantum state be converted into light, transmitted, and written back into another atom.
The potential impact of the work extends beyond quantum computing. Due to its versatility and scalability, it could be adapted for other wavelengths that serve ultra-compact lasers, spectroscopic sensors, and integrated photonics in which many optical resonators can be built directly onto chips.
For more information: Optica
Image: Microcavities of two different lengths, 45 microns and 1 millimeter, placed on a finger tip.