Researchers are pushing the limits of electron microscopy into the tens of picometer scale, a fraction of the size of a hydrogen atom. The ability to see at this subatomic level is crucial for designing new materials with unprecedented properties, such as materials that transition from metals to semiconductors or that exhibit superconductivity.
“This research is important because it highlights our ability to design new classes of materials that can be tuned, one atomic layer at a time, to get interesting new properties such as high-frequency tunable dielectrics, which are of interest to the semiconductor industry,” says Greg Stone, a former Penn State, State College, postdoctoral scholar who is now at the U.S. Army Research, Development, and Engineering Center, Vicksburg, Miss.
Designing new materials with potentially useful properties requires the close collaboration of theory, synthesis, and characterization—the first to build the mathematical models needed, the second to create the material in the lab, and the third to visualize and measure the material’s properties and provide feedback to tweak theories and improve synthesis.
This research builds on previous theoretical work by Turan Birol and Craig Fennie of Cornell University, Ithaca, N.Y., and experimental work by Venkatraman Gopalan of Penn State and Darrell Schlom, formerly at Penn State and now at Cornell, and their students. Gopalan and Nasim Alem, professors of materials science and engineering at Penn State, led the current research.
“The material we are looking at is a form of strontium titanate called a layered oxide,” says Gopalan. “This study brings together electron microscopy and density functional theory on a 5 to 10 picometer length scale to show why these materials are such good tunable dielectrics. “The key is phase competition, and for the first time, we show that many polar phases with similar energies compete in this material on the atomic scale, just as theory predicted, which gives it large tunability under a voltage.”
Complex oxides are materials that form by combining negatively charged oxygen and two other positively charged ions. In this instance, the team examined strontium titanate with a structure called Ruddlesden-Popper (RP), after the two scientists who discovered it.
The structure looks like a brick and mortar wall, with the bricks made of the strontium titanate and the thin mortar between the bricks made up of strontium oxide. When the bricks are layered in this fashion, new properties emerge that would not appear in a single brick.
“In the case of RP-strontium titanate, the emergent property is ferroelectricity, which means it has a built-in electrical polarization within its structure,” says Gopalan. “But it could be magnetism or metal-insulator transitions or superconductivity, depending on the atoms involved and the layering order of the materials.”
Because each layer of brick has a weak connection to other layers, the material can have competing states, with one layer polarized in a direction opposite to a neighboring layer. These competing states result in a material with a strong response to a small external stimulus, such as an electric or magnetic field or temperature. In the case of strontium titanate, there is a large dielectric response, which is the ability to store large amounts of energy, as in a capacitor.
Cell phones have many dielectric components that are very small and have to hold a charge. As cell phones transition from 4G networks to 5G, which means they are processing at 5 billion cycles per second, better materials that respond at higher frequencies are crucial. RP-strontium titanate is a material that is definitely superior to current materials.
Researchers from Penn State, the Molecular Foundry at Lawrence Berkeley National Laboratory collaborated on the project, which was funded in part by the U.S. Deparment of Energy.