Seco Vacuum Technologies, Meadville, Pa., announces that a large North American heat treater has expanded its capabilities by adding a new ZeroFlow precision gas nitriding vacuum furnace. This horizontal, front-loading furnace is designed specifically for precision gas nitriding, ferritic nitrocarburizing, and post oxidation, in a retort-style furnace with vacuum purge.
The new furnace complements a prior Seco Warwick gas nitriding furnace already in production. It extends the customer’s capabilities by offering greater capacity to its growing nitriding customer base. Among its many benefits, the ZeroFlow® gas nitriding method precisely controls the case depth and nitride layer formation including white layer, achieving high surface hardness, improved wear resistance, and longer fatigue life.
Only Seco Vacuum offers the proprietary ZeroFlow control technology. The combination of vacuum purge and ammonia-only process gas reduces gas usage and emissions. SVT’s gas nitriding furnaces achieve optimum results by uniform high convection heating and precision nitriding potential control. Along with vacuum purging, the operating cost reductions and repeatable quality are unmatched for nitriding a variety of metals.