A new technology solution that will provide low-power systems for use in bionic eyes, has been jointly developed by academics from the Harbin Institute of Technology and Northumbria University.
The team discovered that injecting elements of the soft metal, indium, into a two-dimensional (2D) material called molybdenum disulfide (MoS2), could improve electrical conductivity and reduce power consumption of the optical synapses used in the development of bionic eyes.
The technology was then tested within the structure of an electronic retina and found to produce the high-quality image sensing functions required
Professor Fu, professor in Smart Materials and Microsystems at Northumbria’s department of Mathematics, Physics and Electrical Engineering said, “The current visual systems are based on physically separated sensors, memories, and processing units. These systems often have high power consumption and difficulties of performing complex image learning and processing tasks. Therefore, our newly developed method is of great significance for the next generation artificial visual systems.”
Bionic eye implants work inside the existing eye structures or in the brain. They are designed to achieve functional vision goals — as opposed to physical, cosmetic ones. Several bionic eye implants are in development, but currently very few are available, and are suitable only for blindness caused by specific eye diseases. However, as research continues, more and more people may soon benefit from high-tech bionic eyes.
The team’s work has been published in a paper called “Ultralow Power Optical Synapses Based on MoS2 Layers by Indium-Induced Surface Charge Doping for Biomimetic Eyes,” in the scientific journal, Advanced Materials.
For more information: Advanced Materials