Burpee Materials Technology, Eatontown, N.J., specializes in high-yield, high-quality manufacturing of stents and stent-like devices and components. Expertise ranges from fine neurovascular and coronary devices to large AAA/TAA and valve components fabricated from Nitinol, cobalt-chrome, stainless steel, and other biocompatible metals.
Capabilities include state-of-the-art laser machining from tubing, world-class surface finishing, electropolishing to achieve mirror smooth highly passive surfaces, and precision deburring, polishing and chemical etching operations. Other capabilities include wire forming, radiopaque marking, laser welding, and machining.
The company also provides Nitinol forming/shape setting, and features a wide size range of devices and complex shapes that are optimized for mechanical and transition behavior .